Characteristics according to the Amount of HAp Added in Resin for Tooth Repair

문서 유형
연구출판물 · 리뷰논문
등재
KCISCIEScopus
저널 순위
Scopus Q3
저널
JOURNAL OF THE KOREAN CERAMIC SOCIETY56(6) · pp.521 · 2019
피인용
Web of Science 1Scopus 1KCI 1
FWCI (Scopus)
0.02
ISSN
1229-7801

저자

  1. 황승구제1저자Department of Nanomechatronics Engineering, Pusan National University, Busan 46241, Korea
  2. 임진혁Department of Nanomechatronics Engineering, Pusan National University, Busan 46241, Korea
  3. 류수착교신저자Department of Nanomechatronics Engineering, Pusan National University, Busan 46241, Korea

초록

A study was conducted to investigate the possibility of a composite material containing a composite resin as a matrix and hydroxyapatite (HAp) powder as a substitute material for tooth repair. As the content of HAp increased, hardness value (111.9 HV at 9%) increased and flexural strength (73.3 MPa at 9%) decreased. Observation of the microstructure after immersion in a simulated body fluid (SBF) solution confirmed a dense structure due to mutual coagulation and curing. It was thought that fine HAp recrystals were formed with the lapse of time, and they were entangled to form a condensation structure and had a dense structure. In addition, since the activity was shown by the ion migration on the surface of a tooth, it was highly likely that a biocompatible bond occurred during tooth contact. Therefore, it could be used as a substitute material for tooth repair.

키워드

HydroxyapatiteCompositeRepairResinTooth