Effect of cooling rate on hardness and microstructure of Pd-Ag-In-Sn-Ga alloy during porcelain firing simulation
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 피인용
- Web of Science 10Scopus 9
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 3.372
- ISSN
- 1751-6161
저자
- 신혜정제1저자Department of Dental Materials, Institute of Translational Dental Science and BK21 PLUS Project, School of Dentistry, Pusan National University, Beomeo-Ri, Mulgeum-Eup, Yangsan-Si, Gyeongsangnam-Do, 626-814, South Korea
- 권용훈Department of Dental Materials, Institute of Translational Dental Science and BK21 PLUS Project, School of Dentistry, Pusan National University, Beomeo-Ri, Mulgeum-Eup, Yangsan-Si, Gyeongsangnam-Do, 626-814, South Korea
- 설효정교신저자Department of Dental Materials, Institute of Translational Dental Science and BK21 PLUS Project, School of Dentistry, Pusan National University, Beomeo-Ri, Mulgeum-Eup, Yangsan-Si, Gyeongsangnam-Do, 626-814, South Korea
초록
This study examined the effect of the cooling rate on the hardness and its effect on the microstructure during porcelain firing simulation of a Pd-Ag-In-Sn-Ga metal-ceramic alloy. In practice, after each firing step for porcelain bonding, the prosthesis is cooled to room temperature before proceeding to the next firing step. The cooling step is known to allow the hardness of the metal substructure to increase. The aim of the study was to determine whether controlling the cooling rate after each porcelain-firing step increases the hardness of the Pd-Ag-based metal-ceramic alloy. The results showed that the hardness of specimens cooled at a higher cooling rate increased after each firing step compared to specimens cooled at a lower cooling rate (p < 0.05). During cooling after the firing simulation the InPd3-based phase of tetragonal structure precipitated from the Pd-Ag-rich matrix of the face-centered cubic structure. Hardening by cooling at a higher cooling rate after firing was the result of the coherency strains that formed at the interface of the Pd-Ag-rich matrix and the metastable phase based on the InPd3 phase. . The reduced hardness obtained in the specimen cooled at a lower cooling rate after firing resulted from the loss of coherency strains as the fine metastable phases based on the InPd3 phase were transformed into the coarser stable phase with decreased (c/a) of 0.88. This finding revealed that controlling the cooling rate during porcelain firing simulation improves the hardness of the Pd-Ag-In-Sn-Ga metal-ceramic alloy without an additional heat treatment of the alloy.
키워드
Porcelain-firing simulationPd-Ag-In-Sn-Ga alloyCooling rate controlPrecipitationMetastable phaseOXIDATIONPLATINUMBEHAVIORPd–Ag–In–Sn−Ga alloy
식별자
- Scopus EID
- 2-s2.0-85083674946
- WoS UID
- 000530587600008