High-temperature thermal stability and oxidation resistance of Cr and Ta co-alloyed Ti - Al - N coatings deposited by cathodic arc evaporation
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- CORROSION SCIENCE167 · 2020
- 피인용
- Web of Science 50Scopus 53
- FWCI (Scopus)
- 0
- JCR IF
- JCR 2019 6.479
- ISSN
- 0010-938X
저자
- Peng, Bin제1저자a School of Electromechanical Engineering, Guangdong University of Technology, Guangzhou 510006, China
- Li, Haiqinga School of Electromechanical Engineering, Guangdong University of Technology, Guangzhou 510006, China
- Zhang, Quana School of Electromechanical Engineering, Guangdong University of Technology, Guangzhou 510006, China
- Xu, Yu X.교신저자a School of Electromechanical Engineering, Guangdong University of Technology, Guangzhou 510006, China
- Wei, Tiefengb AT&M Six Nine Materials Co., LTD, Beijing 100081, China
- Wang, Qimina School of Electromechanical Engineering, Guangdong University of Technology, Guangzhou 510006, China
- Zhang, Fenggeb AT&M Six Nine Materials Co., LTD, Beijing 100081, China
- 김광호c Global Frontier R&D Center for Hybrid Interface Materials, Pusan National University, Busan 609-735, Korea
초록
Cr and Ta co-alloyed Ti - Al - N coatings were synthesised by cathodic arc deposition. The high-temperature stability and oxidation behaviour of the coatings were investigated by annealing in an inert atmosphere and oxidation environment, respectively. The results indicated that FCC-structured (Ti, Al, Cr, Ta)N coatings exhibit spinodal decomposition and age-hardening upon annealing. Ta retarded the formation of wurtzite A1N and helped to maintain high coating hardness at 900-1000 degrees C. Cr promoted the formation of protective (Al, Cr)(2)O-3 scale and (Ti, Ta)O-2 rutile oxide was found beneath, which reduced mass transport of oxygen during oxidation. Co-alloying with Cr and Ta leads to optimal oxidation resistance of (Ti, Al, Cr, Ta)N coatings.
키워드
CeramicXRDTEMHardeningOxidationMECHANICAL-PROPERTIESSPUTTERED TIPERFORMANCEMICROSTRUCTURETIALNKINETICSFILMSA. CeramicB. TEMB. XRDC. HardeningC. Oxidation
식별자
- Scopus EID
- 2-s2.0-85078742416
- WoS UID
- 000525869800012



로그인
연구물 목록으로