본문 바로가기

Isothermal Phase Transformations and Stability of Retained Austenite during Quenching and Partitioning Process for 0.15C Steel

문서 유형
연구출판물 · 학술지 논문
등재
KCI
저널
대한용접접합학회지35(1) · pp.89 · 2017
피인용
KCI 1
ISSN
2466-2232

저자

  1. 진종원제1저자현대제철
  2. 박철호부산대학교
  3. 강남현교신저자부산대학교

초록

The microstructure and dilatation for 0.15C steels were investigated to define the phase transformation during the quenching and partitioning (Q&P) process. For the one step Q&P dilatation, the isothermal martensite/ bainite transformation occurred because the holding temperature was between Ms and Mf. The isothermally transformed martensite/bainite and the athermally transformed martensite were produced by a loss of retained austenite. As the holding time increased, new martensite-start (Ms) temperature produced from the final quenching process decreased due to the carbon partitioning from the martensite to the retained austenite. This was the direct evidence of increment for the retained austenite stability. For the two step Q&P dilatation, the isothermal bainitic transformation occurred because the partitioning temperature was larger than the Ms and new Ms. The partitioning at 400℃ indicated the short incubation period for the bainite transformation than the 350℃ partitioning because the partitioning at 400℃ should acquire the larger thermal driving force for carbon partitioning than the 350℃ partitioning. A quick drop of Ms and short period of bainite incubation for the 400℃ partitioning steel were also the direct evidence of significant effects of carbon partitioning on the stability of retained austenite.

키워드

Retained austenitePartitioningIsothermal martensite transformationBainite transformationCarbon diffusion

식별자

KCI
ART002201056