본문 바로가기

타액으로 오염된 지르코니아 수복물의 접착강도에 세척 방법들이 미치는 영향

The effect of cleaning methods on bond strength of zirconia after saliva contamination

문서 유형
연구출판물 · 학술지 논문
등재
KCI
저널
대한치과재료학회지44(1) · pp.61 · 2017
피인용
KCI 0
ISSN
2384-4434

저자

  1. 심영보제1저자부산대학교 치의학전문대학원
  2. 최안나부산대학교 치의학전문대학원
  3. 손성애부산대학교 치의학전문대학원
  4. 정경화부산대학교 치의학전문대학원
  5. 권용훈부산대학교 치의학전문대학원
  6. 박정길교신저자부산대학교 치의학전문대학원

초록

This study evaluated the effects of various cleaning methods on the shear bond strength of zirconia ceramics after saliva contamination. Eighty zirconia disk specimens were divided into 8 groups. All groups were treated with one coat of MDP primer. All specimens (except the negative control) were contaminated with human saliva on the zirconia surface. The positive control went through the bonding procedure immediately after contamination without any cleaning procedure. With the exception of control groups, the remaining six groups were rinsed with water and either applied with MDP recoating (WATER+MDP) or without MDP recoating (WATER). While some were cleaned with a Ivoclean with MDP recoating (IVOCLEAN+MDP) or not applied with MDP recoating(IVOCLEAN), others were cleaned with a 1% NaOCl solution with MDP recoating (NaOCl+MDP) or without MDP recoating (NaOCl). The shear bond strength of all specimens were measured after being stored in distilled water at 37°C for 24 hours. The data was analyzed statistically by an analysis of ANOVA, Tukey’s post hoc test and Student’s t-test was used to compare the shear bond strength according to the re-coating of MDP after the cleaning procedure. The positive control group showed the lowest shear bond strength value, and the WATER group and NaOCl group showed no significant difference when compared to the positive control group. The IVOCLEAN group showed significantly higher shear bond strength when compared to Water group and NaOCl group but not with the group of negative control. After rinsing with water or the NaOCl solution, the comparison of the single coating of MDP and re-coating of MDP showed different shear bond strengths but there was no significant difference to the negative control. After rinsing with Ivoclean, there was no significant difference to the negative control regardless of the recoating of MDP. In conclusion, the shear bond strength was affected by the cleansing procedure and Ivoclean was found to be effective regardless of the re-coating of MDP. When water or the NaOCl solution is used to remove surface contaminants, the re-coating of MDP provides a positive effect on cementation.

키워드

ZirconiaSalivaCleaningNaOClIvocleanShear bond strength

식별자

KCI
ART002211227