저자
- 정제기제1저자Department of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- 조의제Department of Materials Science and Engineering, Virginia Polytechnic Institute and State University, Blacksburg, VA 24061, USA
- Kim, Su-Hyeon교신저자Metallic Materials Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- Lee, Yun-SooMetallic Materials Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- 김희주Department of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
- Lim, Cha-YongMetallic Materials Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
- 박용호Department of Materials Science and Engineering, Pusan National University, Busan 46241, Republic of Korea
초록
The ballistic performances and deformation behaviors of AA5052-H112, AA5083-H112, AA6061-T6, and AA7075-T651 aluminum alloy plates struck by 7.62 mm armor piercing projectiles were investigated. Ballistic impact tests were performed using 25 mm thick aluminum alloy plates with different projectile velocities to obtain the ballistic limit velocity (V-50). Microstructural and mechanical responses to the ballistic impacts were studied using optical microscopy, electron backscattered diffraction, transmission electron microscopy, and hardness measurements. Finite element analysis was performed to simulate the deformation behavior of the materials of interest. The ballistic limit velocity exhibited a linear relationship with the hardness and yield strength of the alloys, but not with the tensile strength or elongation. Ductile hole formation and strain hardening were observed in the AA5052-H112 and AA5083-H112 alloy plates, whereas AA6061-T6 exhibited both strain hardening and softening behaviors. The AA7075-T651 plate failed by a spalling mechanism accompanied by formation of adiabatic shear bands.
키워드
Aluminum alloysBallistic impactDeformation behaviorMicrostructureStrain hardeningStrain softeningADIABATIC SHEAR BANDSMG-CU ALLOYNOSE STEEL PROJECTILESFRICTION STIR WELDSHIGH-STRAIN-RATECONSTITUTIVE BEHAVIORCORROSION BEHAVIORHEAT-TREATMENTPLATESPERFORATION