본문 바로가기

Preparation and properties of flame-retardant epoxy resins containing reactive phosphorus flame retardant

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q3Scopus Q4
피인용
Web of Science 18Scopus 18
FWCI (Scopus)
0
JCR IF
JCR 2019 0.814
ISSN
1558-9250

저자

  1. 이상훈제1저자Department of Organic Material Science and Engineering, College of Engineering, Pusan National University, Busan, Korea
  2. 오승원Department of Organic Material Science and Engineering, College of Engineering, Pusan National University, Busan, Korea
  3. 이영희Department of Organic Material Science and Engineering, College of Engineering, Pusan National University, Busan, Korea
  4. Kim, Il-JinKorea Institute of Footwear Leather Technology, Busan, Korea
  5. Lee, Dong-JinKorea Institute of Footwear Leather Technology, Busan, Korea
  6. Lim, Jae-ChunHyundai Fiber Co, Ltd, Yangsan-si, Korea
  7. Park, Cha-CheolLibral Arts College, Dongseo University, Busan, Korea
  8. 김한도교신저자Department of Organic Material Science and Engineering, College of Engineering, Pusan National University, Busan, Korea

초록

To prepare flame-retardant epoxy resin, phosphorus compound containing di-hydroxyl group (10-(2,5-dihydroxyphenyl)-9,10-dihydro-9-oxa-10-phospha phenanthrene-10-oxide, DOPO-HQ) was reacted with uncured epoxy resin (diglycidyl ether of bisphenol A, YD-128) and then cured using a curing agent (dicyandiamide, DICY). This study focused on the effect of phosphorus compound/phosphorus content on physical properties and flame retardancy of cured epoxy resin. The thermal decomposition temperature of the cured epoxy resins (samples: P0, P1.5, P2.0, and P2.5, the number represents the wt% of phosphorus) increased with increasing the content of phosphorus compound/phosphorus (0/0, 19.8/1.5, 27.8/2.0, and 36.8/2.5 wt%) based on epoxy resin. The impact strength of the cured epoxy resin increased significantly with increasing phosphorus compound content. As the phosphorus compound/phosphorus content increased from 0/0 to 36.8/2.5 wt%, the glass transition temperature (the peak temperature of loss modulus curve) increased from 135.2 degrees C to 142.0 degrees C. In addition, as the content of phosphorous compound increased, the storage modulus remained almost constant up to higher temperature. The limiting oxygen index value of cured epoxy resin increased from 21.1% to 30.0% with increasing phosphorus compound/phosphorus content from 0/0 to 36.8/2.5 wt%. The UL 94 V test result showed that no rating for phosphorus compounds less than 19.8 wt% and V-1 for 27.8 wt%. However, when the phosphorus compound was 36.8 wt%, the V-0 level indicating complete flame retardancy was obtained. In conclusion, the incorporation of phosphorus compounds into the epoxy chain resulted in improved properties such as impact strength and heat resistance, as well as a significant increase in flame retardancy.

키워드

Halogen-free flame-retardant epoxy resinphosphorus compoundUL 94 Vlimiting oxygen index

식별자

Scopus EID
2-s2.0-85078182187
WoS UID
000509579600001