Synthesis and Characterization of Hollow Glass Sphere Containing Aluminum Syntactic Foam by Spark Plasma Sintering and Hot Pressing

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q3
저널
METALS9(12) · 2019
피인용
Web of Science 4Scopus 6
FWCI (Scopus)
0.17
JCR IF
JCR 2018 2.259
ISSN
2075-4701

저자

  1. 손용국제1저자Department of Materials Science and Engineering, Pusan National University, 2 Busandaehak-ro 63 beongil, Busan 46241, Korea
  2. Lee, Young CheolKorea Institute of Industrial Technology (KITECH), 42-7 Baegyang-daero 804 beon-gil, Busan 46938, Korea
  3. 정성수Korea Institute of Industrial Technology (KITECH), 42-7 Baegyang-daero 804 beon-gil, Busan 46938, Korea
  4. Kwon, Han SangDepartment of Materials System Engineering, Pukyong National University, 365 Sinseon-ro Nam-gu 48547, Busan 608737, Korea
  5. 이욱진교신저자Korea Institute of Industrial Technology (KITECH), 42-7 Baegyang-daero 804 beon-gil, Busan 46938, Korea
  6. 박용호Department of Materials Science and Engineering, Pusan National University, 2 Busandaehak-ro 63 beongil, Busan 46241, Korea

초록

The effect of sintering process on the microstructure and the mechanical properties of aluminum syntactic foam were investigated in this study. Two different sintering processes of spark plasma sintering and hot pressing were used. Glass hollow spheres with a size of 50-80 mu m was used to fabricate the foams having various volume fractions of the spheres in the range of 10-30%. Microstructural analysis revealed that the glass hollow spheres were uniformly distributed in the aluminum matrix, both in the spark plasma sintered and hot pressed ones. As the volume fraction of the spheres increased from 10 to 30%, the density, micro-hardness and compressive strength of the foams were decreased. In comparison to the foams fabricated by hot pressing method, the spark plasma sintered foams had slightly lower density and mechanical strength. In nanoindentation study, it was found that the aluminum matrix in the foam prepared by the spark plasma sintering process had lower strength than foam prepared by the hot pressing process. This is likely because of shorter sintering time used in the spark plasma sintering process than the hot pressing.

키워드

aluminum syntactic foamspark plasm sinteringglass hollow spheremicrostructuremechanical propertiesMECHANICAL-PROPERTIESBEHAVIORALMICROSTRUCTURECOMPOSITESFABRICATION