7003 알루미늄 합금의 기계적 성질 및 에너지 흡수능에 미치는 열처리 조건의 영향

Effect of Heat Treatment on Mechanical Properties and Energy Absorption Capacity of 7003 Aluminum Alloy

문서 유형
연구출판물 · 학술지 논문
등재
KCISCIEScopus
저널 순위
JCR Q3Scopus Q2
저널
Korean Journal of Metals and Materials58(1) · pp.7 · 2020
피인용
Web of Science 6Scopus 7KCI 6
FWCI (Scopus)
0
JCR IF
JCR 2019 1.146
ISSN
1738-8228

저자

  1. 김희주제1저자Department of Materials Science and Engineering, Pusan National University, Busan 46269, Republic of Korea
  2. 정제기Department of Materials Science and Engineering, Pusan National University, Busan 46269, Republic of Korea
  3. Kim, Su-Hyeon교신저자Metallic Materials Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
  4. Lim, Cha-YongMetallic Materials Division, Korea Institute of Materials Science, Changwon 51508, Republic of Korea
  5. 최윤석Department of Materials Science and Engineering, Pusan National University, Busan 46269, Republic of Korea

초록

The effects of heat treatment conditions on the mechanical properties and energy absorption capacity of 7003 (Al-6Zn-0.6Mg) aluminum alloy were studied. The extruded material was heat treated at various temperatures to prepare annealed or aged specimens. Tensile tests, hardness measurements, electron backscatter diffraction characterizations, and differential scanning calorimeter analyses were carried out to investigate the mechanical properties and microstructures of the as-extruded or heat treated specimens. Axial compression tests of circular tube samples were also performed to characterize their energy absorption behavior. Specific energy absorption was calculated by measuring the absorbed energy per unit weight of the tube specimen. The peak reaction force was defined as the maximum force applied during the compression test. The as-extruded material with high strength and low elongation exhibited fracture failure during the axial compression test. After a low temperature annealing at 200 or 250 degrees C, the material had low strength and low energy absorption capacity. In contrast, the high temperature (300 to 400 degrees C) heat treatment resulted in an increase in strength and enhancement of energy absorption capacity. The aging treatment effectively increased the strength and the energy absorption capacity. After artificial aging, fine and uniform precipitates were formed. The artificially aged specimens showed the highest yield strength and therefore exhibited the highest energy absorption capacity among the heat treated specimens. Specific energy absorption and peak reaction force were linearly proportional to the flow stress of the material.

키워드

Al-Zn-Mg alloyheat treatmentenergy absorption capacitymechanical propertiesmicrostructureZN-MG ALLOYTEMPERATUREPERFORMANCEABSORBERSEVOLUTIONCOLLAPSEBEHAVIORSHEET

식별자

Scopus EID
2-s2.0-85078210827
WoS UID
000506216700002
KCI
ART002547561