Accelerating heterogeneous nucleation to increase hardness and electrical conductivity by deformation prior to ageing for Cu-4 at.% Ti alloy
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q3Scopus Q3
- 저널
- PHILOSOPHICAL MAGAZINE LETTERS99(8) · pp.275 · 2019
- 피인용
- Web of Science 12Scopus 13
- FWCI (Scopus)
- 0.37
- JCR IF
- JCR 2018 1.117
- ISSN
- 0950-0839
저자
- Han, Seung Zeon제1저자Computational Materials Department, Korea Institute of Materials Science, Changwon, Korea
- Semboshi, SatoshiTrans-Regional Corporation Center for Industrial Materials Research, Tohoku University, Sendai, Japan
- Ahn, Jee HyukComputational Materials Department, Korea Institute of Materials Science, Changwon, Korea
- Choi, Eun-AeComputational Materials Department, Korea Institute of Materials Science, Changwon, Korea
- 조민아School of Materials Science and Engineering, Pusan National University, Busan, Korea
- Kadoi, YusukeTrans-Regional Corporation Center for Industrial Materials Research, Tohoku University, Sendai, Japan
- 김광호School of Materials Science and Engineering, Pusan National University, Busan, Korea
- Lee, Jehyun교신저자Department of Materials Science and Engineering, Changwon National University, Changwon, Korea
초록
Deformation bands, especially shear bands were intentionally formed in supersaturated Cu-4 at.% Ti alloy by groove-rolling with 75% area reduction. Cold deformation prior to the ageing process changed the precipitation behaviour of the alloy. The deformed structure with shear bands was maintained, without showing recovery and recrystallisation, even after prolonged ageing at 450?C for more than one day. The thermally stable shear bands act as nucleation initiation sites and prevent the expansion of discontinuous cellular precipitates. The hardness reached a value of 305?Hv and an electrical conductivity of 15% IACS (IACS?=?International Annealed Copper Standard. 100% IACS is defined as the conductivity corresponding to a volume resistivity at 20?C of 17.241?n?), compared to 283?Hv and 13% IACS for conventional solid-solutioned and peak-hardened alloy. In addition, the ageing time to reach the highest hardness was shortened from 720 to 180?min at 450?C.
키워드
Copper-titanium alloysshear banddiscontinuous precipitationheterogeneous nucleationelectrical conductivityDISCONTINUOUS PRECIPITATIONTITANIUMCOPPERTENSILE