Hydrogen-Induced Cracking of Laser Beam and Gas Metal Arc Welds on API X65 Steel
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q3Scopus Q2
- 저널
- Korean Journal of Metals and Materials57(8) · pp.491 · 2019
- 피인용
- Web of Science 10Scopus 11KCI 7
- FWCI (Scopus)
- 0.65
- JCR IF
- JCR 2018 0.992
- ISSN
- 1738-8228
저자
- 이정훈제1저자Department of Materials Science and Engineering, Pusan National University, Busan, 46241, Republic of Korea
- 김명현Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, 46241, Republic of Korea
- Park, YeongdoDepartment of Advanced Materials Engineering, Dong-Eui University, Busan, 47340, Republic of Korea
- Park, CheolhoKorea Atomic Energy Research Institute, Daejeon, 34057, Republic of Korea
- Kim, CheolheeJoining R&D group, Korea Institute of Industrial Technology, Incheon, 21999, Republic of Korea
- 강남현교신저자Department of Materials Science and Engineering, Pusan National University, Busan, 46241, Republic of Korea
초록
Hydrogen-induced cracking (HIC) behavior was analyzed for gas metal arc (GMA) and laser beam (LB) welds on American Petroleum Institute (API) X65 steel. The GMA welds consisted of acicular ferrite (AF) with some widmanstatten ferrite (WF), while the LB welds had bainitic ferrite (BF) with some AF. The welds and heat affected zone (HAZ) of GMA exhibited a hardness of 220-250 HV, while those of the LB had a hardness of 230-290 HV. The LB welds and HAZ exceeded the hardness limit of 250 HV for pipeline steel, defined by the National Association of Corrosion Engineers (NACE) standard. Slow strain rate tests (SSRT) were performed in air and in-situ with hydrogen to observe HIC behavior. The ultimate tensile strength of the GMA welds decreased by 13%, while that of the LB welds decreased by 16% after hydrogen charging. Both welds showed a dimple fracture in the center and quasi-cleavage fracture along the edges. When austenite transforms to BF, it is known to grow along the directions of twins or the Kurdjumov-Sachs relation. These directions are strongly related to the coincidence site lattice, specifically Sigma 3 and Sigma 13b, and have good crack resistance. Because of this grain boundary characteristic, the LB welds with a BF microstructure showed good HIC behavior compared to the GMA welds.
키워드
pipeline steelhydrogen-induced crackingcoincidence site latticegas metal arc weldlaser beam weldSULFIDE STRESS CRACKINGPIPELINE STEELSGRAIN-BOUNDARYCRYSTALLOGRAPHIC TEXTURECORROSION CRACKINGX70RESISTANCEMICROSTRUCTURESUSCEPTIBILITYPERMEATION