Hydration of Calcium Sulfoaluminate-Based Binder Incorporating Red Mud and Silica Fume
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- APPLIED SCIENCES-BASEL9(11) · 2019
- 피인용
- Web of Science 14Scopus 16
- FWCI (Scopus)
- 0.53
- JCR IF
- JCR 2018 2.217
- ISSN
- 2076-3417
저자
- Jun, Yubin제1저자Department of Civil and Environmental Engineering, Korea Advanced Institute of Science and Technology, Daejeon 34141, Korea; ssjun97@gmail.com (Y.J.); jae.kim@kaist.ac.kr (J.H.K.)
- Kim, Jae HongDepartment of Civil and Environmental Engineering, Korea Advanced Institute of Science and Technology, Daejeon 34141, Korea; ssjun97@gmail.com (Y.J.); jae.kim@kaist.ac.kr (J.H.K.)
- 김태완교신저자Department of Civil Engineering, Pusan National University, Busan 46241, Korea; ring2014@naver.com
초록
This study investigated the properties of hardened pastes made with calcium sulfoaluminate expansive agent (CSA), red mud, and silica fume. Five different ratios of 10:90, 20:80, 30:70, 40:60, and 50:50 were applied as the weight ratios of CSA and red mud. Red mud was replaced with 0, 5, and 10% silica fume by weight. Compressive strength, drying shrinkage, XRD, MIP, and SEM/EDS of the hardened pastes were performed. The results indicated that as the amount of CSA increased (i.e., as the amount of red mud decreased) up to 30%, sample strengths showed a tendency to increase. The main reaction product of the pastes was expansive ettringite, which was formed from the consumption of ye'elimite, anhydrite, gypsum, and Ca(OH)(2). It was expected that C-S-H would be formed by the reaction of C2S in red mud; however, C-S-H phase was not present, and the pozzolanic activity due to the use of silica fume did not occur. The increase of CSA replacement level was effective for controlling the drying shrinkage of the samples. However, 50% replacement level of CSA induced excessive expansion, leading to the reduction in strength. It was found that the excessive expansion in the sample was reduced by the addition of silica fume.
키워드
calcium sulfoaluminatered mudsilica fumeby-productettringiteye'elimiteSTRENGTH DEVELOPMENTETTRINGITECEMENTGYPSUMMICROSTRUCTUREPERFORMANCEMECHANISMSEXPANSIONKINETICSRATIO