Hydrogen reduction behavior and microstructural characteristics of WO3 and WO3-NiO powders

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q1
피인용
Web of Science 19Scopus 21
FWCI (Scopus)
0.69
JCR IF
JCR 2018 2.794
ISSN
0263-4368

저자

  1. Kang, Hyunji제1저자Department of Materials Science and Engineering, Seoul National University of Science and Technology, Seoul, South Korea
  2. 정영근Graduate School of Convergence Science, Pusan National University, Busan, South Korea
  3. Oh, Sung-Tag교신저자Department of Materials Science and Engineering, Seoul National University of Science and Technology, Seoul, South Korea

초록

The characterization and understanding of the hydrogen reduction and sintering behavior of powder mixtures prepared from WO3 and WO3-NiO have been investigated. The nano-sized W and W-Ni powders were prepared by ball milling and hydrogen reduction of oxide powders. The reduction behavior is analyzed by temperature programmed reduction method with different heating rates in Ar-10% H-2 atmosphere. X-ray diffractometry analysis revealed that the oxide powders are changed to W and W-Ni powders with an average particle size of about 100 nm by hydrogen reduction at 800 degrees C for 1 h. The hydrogen reduction kinetics was evaluated by the amount of peak shift with heating rates. The activation energies for the reduction of pure WO3 and WO3-NiO, estimated by the slope of the Kissinger plot, were measured as 87.4-117.4 kJ/mol depending on reduction steps. The consolidated W-Ni by spark plasma sintering has relatively dense and large grains with neck growth by enhanced mass transport due to the addition of Ni. These results are help to optimize the powder synthesis process and to understand the hydrogen reduction behavior and Ni addition effect related to microstructure of powders and sintered bodies.

키워드

W and W-NiMetal oxidesHydrogen reduction behaviorSpark plasma sinteringMicrostructureGRAIN-GROWTHTUNGSTENDENSIFICATIONNANOOXIDE