본문 바로가기

Coupling material characteristics with water-cement ratio for elastic wave based monitoring of underground structure

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q1
피인용
Web of Science 15Scopus 15
FWCI (Scopus)
0.34
JCR IF
JCR 2018 3.942
ISSN
0886-7798

저자

  1. 이종원제1저자Multi Disaster Countermeasure Organization, Korea Institute of Geoscience and Mineral Resources (KIGAM), Daejeon, South Korea
  2. 오태민교신저자Department of Civil Engineering, Pusan National University (PNU), Busan, South Korea
  3. Kim, HyunwooMulti Disaster Countermeasure Organization, Korea Institute of Geoscience and Mineral Resources (KIGAM), Daejeon, South Korea
  4. Kim, Min-KoanDepartment of Civil Engineering Geotechnical Engineering Group, Yokohama National University (YNU), Yokohama, Japan

초록

Elastic wave based technology (e.g., acoustic emission or micro seismic sensors) has been widely used to monitor the stability of underground structures or rock failure. To achieve successful measurement, it is important to select an appropriate coupling material for the installation of sensors that are embedded in holes bored into the wall of a structure. The characteristics of the coupling material are related to its wave propagation ability (i.e., wave velocity and damping ratio), setting ability in the borehole (i.e., bleeding), and its workability (i.e., viscosity) in relation to being able to fill the holes tightly with the sensors. In this study, micro cement, Portland cement, and gypsum were the materials considered to couple with sensors in the borehole. Laboratory tests were performed to evaluate the characteristics of the coupling material according to the water -cement ratio (w/c, range 0.5-2.0). The test results show that the propagation ability and setting ability tend to decrease with increasing w/c ratio; on the other hand, workability benefits from an increasing w/c ratio. In addition, the characteristics of the coupling materials were analyzed to suggest a material with an optimized w/c ratio appropriate for a target test-bed site. The most suitable coupling recipe was found to be micro cement with a w/c ratio of 1.0. This study provides information about coupling material characteristics that should be useful for determining a suitable coupling recipe for field applications.

키워드

Coupling materialCoupling recipeWater-cement ratioUnderground structure monitoringACOUSTIC-EMISSIONRHEOLOGICAL PROPERTIESWATER/CEMENT RATIOVELOCITYSTRESSGROUTSEXCAVATIONEVOLUTIONVISCOSITYLIMESTONE

식별자

Scopus EID
2-s2.0-85056870670
WoS UID
000457506700011