본문 바로가기

All-Solid-State Lithium Battery Working without an Additional Separator in a Polymeric Electrolyte

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q2
저널
POLYMERS10(12) · 2018
피인용
Web of Science 27Scopus 28
FWCI (Scopus)
0.63
JCR IF
JCR 2017 2.935
ISSN
2073-4360

저자

  1. 조성규제1저자Secondary Battery R and D Center, DRB Holdings Co., Pusan, South Korea
  2. Kim, ShinhoSecondary Battery R and D Center, DRB Holdings Co., Pusan, South Korea
  3. 김원호Department of Chemical and Biochemical Engineering, Pusan National University, Pusan, South Korea
  4. 김석Department of Chemical and Biochemical Engineering, Pusan National University, Pusan, South Korea
  5. Ahn, Sungsook교신저자Secondary Battery R and D Center, DRB Holdings Co., Pusan, South Korea

초록

Considering the safety issues of Li ion batteries, an all-solid-state polymer electrolyte has been one of the promising solutions. Achieving a Li ion conductivity of a solid-state electrolyte comparable to that of a liquid electrolyte (>1 mS/cm) is particularly challenging. Even with characteristic ion conductivity, employment of a polyethylene oxide (PEO) solid electrolyte has not been sufficient due to high crystallinity. In this study, hybrid solid electrolyte (HSE) systems have been designed with Li1.3Al0.3Ti0.7(PO4)(3) (LATP), PEO and lithium bis(trifluoromethanesulfonyl)imide (LiTFSI). A hybrid solid cathode (HSC) is also designed using LATP, PEO and lithium cobalt oxide (LiCoO2, LCO)lithium manganese oxide (LiMn2O4, LMO). The designed HSE system has 2.0 x 10(-4) S/cm (23 degrees C) and 1.6 x 10(-3) S/cm (55 degrees C) with a 6.0 V electrochemical stability without an additional separator membrane introduction. In these systems, succinonitrile (SN) has been incorporated as a plasticizer to reduce crystallinity of PEO for practical all-solid Li battery system development. The designed HSC/HSE/Li metal cell in this study operates without any leakage and short-circuits even under the broken cell condition. The designed HSC/HSE/Li metal cell in this study displays an initial charge capacity of 82/62 mAh/g (23 degrees C) and 123.4/102.7 mAh/g (55 degrees C). The developed system overcomes typical disadvantages of internal resistance induced by Ti ion reduction. This study contributes to a new technology development of all-solid-state Li battery for commercial product design.