Initial oxidation behavior of Fe-Cr-Si alloys in 1200 degrees C steam
Initial oxidation behavior of Fe-Cr-Si alloys in 1200 °C steam
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- JOURNAL OF NUCLEAR MATERIALS513 · pp.297 · 2019
- 피인용
- Web of Science 35Scopus 41
- FWCI (Scopus)
- 1.84
- JCR IF
- JCR 2018 2.547
- ISSN
- 0022-3115
저자
- 문준호제1저자School of Mechanical Engineering, Pusan National University, Busan, South Korea
- 김선규School of Mechanical Engineering, Pusan National University, Busan, South Korea
- 박원동School of Mechanical Engineering, Pusan National University, Busan, South Korea
- Kim, Tae YongDepartment of Nuclear Engineering, School of Mechanical and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Ulsan, South Korea
- McAlpine, Samuel WestcottDept. of Nuclear Science and Engineering, Massachusetts Institute of Technology, Cambridge, United States
- Short, Michael P.Dept. of Nuclear Science and Engineering, Massachusetts Institute of Technology, Cambridge, United States
- Kim, Ji HyunDepartment of Nuclear Engineering, School of Mechanical and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Ulsan, South Korea
- 반치범교신저자School of Mechanical Engineering, Pusan National University, Busan, South Korea
초록
Accident-tolerant fuel (ATF) cladding with high oxidation resistance during severe accidents is of critical importance to light water reactor safety and sustainability. One newly proposed ATF cladding concept, a multi-metallic layered composite (MMLC), hinges upon the oxidation resistance of an outer Fe-Cr-Si layer on top of a Zr-based alloy, separated by barrier layers to avoid Fe-Zr eutectic formation. The initial oxidation resistance of three potential Fe-Cr-Si alloys was evaluated by exposing them to 1200 degrees C oxidizing steam for up to one hundred seconds, along with a Zr-Nb-Sn alloy as a reference. The oxidation resistance of Fe12Cr2Si and Fe16Cr2Si was poor, exhibiting a porous, incomplete multilayer oxide composed mainly of mixed Fe/Cr/Si spinels. However, Fe20Cr2Si showed excellent oxidation resistance due to a continuous amorphous SiO2 layer formed at the metal-oxide interface, followed by almost fully dense Cr2O3. This motivates the consideration of Fe-Cr-Si alloys as an additional ATF design choice, similar to FeCrAl alloys in performance and oxidation resistance mechanism. (C) 2018 Elsevier B.V. All rights reserved.
키워드
Accident-tolerant fuel claddingFe-Cr-Si alloyHigh-temperature oxidation testAmorphous SiO2 layerHIGH-TEMPERATURE OXIDATIONCLADDING CANDIDATE MATERIALSTHERMAL-OXIDATIONOXIDE LAYERFUELDIFFUSIONKINETICSIRONCORROSIONTOLERANT
식별자
- Scopus EID
- 2-s2.0-85055628745
- WoS UID
- 000451783700030



로그인