Enamel Anti-Demineralization Effect of Orthodontic Adhesive Containing Bioactive Glass and Graphene Oxide: An In-Vitro Study
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- MATERIALS11(9) · 2018
- 피인용
- Web of Science 56Scopus 60
- FWCI (Scopus)
- 1.62
- JCR IF
- JCR 2017 2.467
- ISSN
- 1996-1944
저자
- 이승민제1저자Department of Orthodontics, Dental Research Institute, Pusan National University Dental Hospital, Yangsan, South Korea
- 유경현School of Materials Science and Engineering, Pusan National University, Busan, South Korea
- 윤석영School of Materials Science and Engineering, Pusan National University, Busan, South Korea
- 김인령Department of Oral Anatomy, School of Dentistry, Pusan National University, Yangsan, South Korea
- 박봉수Department of Oral Anatomy, School of Dentistry, Pusan National University, Yangsan, South Korea
- 손우성Department of Orthodontics, Dental Research Institute, Pusan National University Dental Hospital, Yangsan, South Korea
- Ko, Ching-ChangDepartment of Orthodontics, School of Dentistry, University of North Carolina at Chapel Hill, Chapel Hill, United States
- 손성애교신저자Department of Conservative Dentistry, School of Dentistry, Pusan National University, Yangsan, South Korea
- 김용일Institute of Translational Dental Sciences, Pusan National University, Busan, South Korea
초록
White spot lesions (WSLs), a side effect of orthodontic treatment, can result in reversible and unaesthetic results. Graphene oxide (GO) with a bioactive glass (BAG) mixture (BAG@GO) was added to Low-Viscosity Transbond XT (LV) in a ratio of 1, 3, and 5%. The composite's characterization and its physical and biological properties were verified with scanning electron microscopy (SEM) and X-ray diffraction (XRD); its microhardness, shear bond strength (SBS), cell viability, and adhesive remnant index (ARI) were also assessed. Efficiency in reducing WSL was evaluated using antibacterial activity of S. mutans. Anti-demineralization was analyzed using a cycle of the acid-base solution. Adhesives with 3 wt.% or 5 wt.% of BAG@GO showed significant increase in microhardness compared with LV. The sample and LV groups showed no significant differences in SBS or ARI. The cell viability test confirmed that none of the sample groups showed higher toxicity compared to the LV group. Antibacterial activity was higher in the 48-h group than in the 24 h group; the 48 h test showed that BAG@GO had a high antibacterial effect, which was more pronounced in 5 wt.% of BAG@GO. Anti-demineralization effect was higher in the BAG@GO-group than in the LV-group; the higher the BAG@GO concentration, the higher the anti-demineralization effect.