Microscopic characterization of pretransition oxide formed on Zr-Nb-Sn alloy under various Zn and dissolved hydrogen concentrations
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q1Scopus Q2
- 저널
- NUCLEAR ENGINEERING AND TECHNOLOGY50(3) · pp.416 · 2018
- 피인용
- Web of Science 4Scopus 5KCI 0
- FWCI (Scopus)
- 0.12
- JCR IF
- JCR 2017 1.655
- ISSN
- 1738-5733
저자
- 김성규제1저자School of Mechanical Engineering, Pusan National University, Busan, South Korea
- Kim, TaehoDepartment of Nuclear Engineering, School of Mechanical, Aerospace and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Ulsan, South Korea
- Kim, Ji HyunDepartment of Nuclear Engineering, School of Mechanical, Aerospace and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Ulsan, South Korea
- 반치범교신저자School of Mechanical Engineering, Pusan National University, Busan, South Korea
초록
Microstructure of oxide formed on Zr-Nb-Sn tube sample was intensively examined by scanning transmission electron microscopy after exposure to simulated primary water chemistry conditions of various concentrations of Zn (0 or 30 ppb) and dissolved hydrogen (H-2) (30 or 50 cc/kg) for various durations without applying desirable heat flux. Microstructural analysis indicated that there was no noticeable change in the microstructure of the oxide corresponding to water chemistry changes within the test duration of 100 days (pretransition stage) and no significant difference in the overall thickness of the oxide layer. Equiaxed grains with nano-size pores along the grain boundaries and microcracks were dominant near the water/oxide interface, regardless of water chemistry conditions. As the metal/oxide interface was approached, the number of pores tended to decrease. However, there was no significant effect of H-2 concentration between 30 cc/kg and 50 cc/kg on the corrosion of the oxide after free immersion in water at 360 degrees C. The adsorption of Zn on the cladding surface was observed by X-ray photoelectron spectroscopy and detected as ZnO on the outer oxide surface. From the perspective of OH - ion diffusion and porosity formation, the absence of noticeable effects was discussed further. (C) 2018 Korean Nuclear Society, Published by Elsevier Korea LLC.
키워드
Dissolved Hydrogen EffectPorosityPretransition OxideTransmission Electron Microscopy (TEM)Zirconium AlloysZIRCONIUM ALLOYSPICK-UPSTABILIZED ZIRCONIACLADDING ALLOYSWATERCORROSIONOXIDATIONDEGRADATIONMECHANISMSPOROSITY
식별자
- Scopus EID
- 2-s2.0-85041597399
- WoS UID
- 000430151900010
- KCI
- ART002337119



로그인
연구물 목록으로