Effects of substrate preheating during direct energy deposition on microstructure, hardness, tensile strength, and notch toughness
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- METALS AND MATERIALS INTERNATIONAL23(6) · pp.1204 · 2017
- 피인용
- Web of Science 36Scopus 38KCI 6
- FWCI (Scopus)
- 1.35
- JCR IF
- JCR 2016 1.889
- ISSN
- 1598-9623
저자
- Baek, Gyeong Yun제1저자Department of Mechanical Engineering, Chonnam National University, Gwangju, South Korea
- Lee, Ki Yong교신저자Green Manufacturing Process Group, KITECH, Gwangju, South Korea
- 박상후Department of Mechanical Engineering, Pusan National University, Busan, South Korea
- Shim, Do SikDivision of Mechanical Engineering, Korea Maritime and Ocean University, Busan, South Korea
초록
This study examined the effects of substrate preheating for the hardfacing of cold-press dies using the high-speed tool steel AISI M4. The preheating of the substrate is a widely used technique for reducing the degree of thermal deformation and preventing crack formation. We investigated the changes in the metallurgical and mechanical properties of the high-speed tool steel M4 deposited on an AISI D2 substrate with changes in the substrate preheating temperature. Five preheating temperatures (100-500 A degrees C; interval of 100 A degrees C) were selected, and the changes in the temperature of the substrate during deposition were observed. As the preheating temperature of the substrate was increased, the temperature gradient between the melting layer and the substrate decreased; this prevented the formation of internal cracks, owing to thermal stress relief. Field-emission scanning electron microscopy showed that a dendritic structure was formed at the interface between the deposited layer and the substrate while a cellular microstructure was formed in the deposited layer. As the preheating temperature was increased, the sizes of the cells and precipitated carbides also increased. Furthermore, the hardness increased slightly while the strength and toughness decreased. Moreover, the tensile and impact properties deteriorated rapidly at excessively high preheating temperatures (greater than 500 A degrees C). The results of this study can be used as preheating criteria for achieving the desired mechanical properties during the hardfacing of dies and molds.
키워드
metalslaser-assisted depositionmechanical propertiesscanning electron microscopy (SEM)WORK TOOL STEELSAISI D2 STEELCRACK FORMATIONHEAT-TREATMENTDIE REPAIRLASERTEMPERATUREBEHAVIORMETALWEAR