본문 바로가기

Thermo-mechanical evolution of ternary Bi-Sn-In solder micropowders and nanoparticles reflowed on a flexible PET substrate

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q1
저널
APPLIED SURFACE SCIENCE415 · pp.28 · 2017
피인용
Web of Science 14
JCR IF
JCR 2016 3.387
ISSN
0169-4332

저자

  1. Kim, Sang Hoon제1저자School of Materials Science and Engineering, Pusan National University, Busan, South Korea
  2. Yang, Dong-YeolPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  3. Kim, Yong-JinPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  4. Min, TaesikPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  5. Choi, JoonphilPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  6. Yun, JaecheolPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  7. Nguyen, Van LuongPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  8. Kim, Ki BongPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  9. Kim, Young JaPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  10. Lee, Jun HongPowder Technology Department, Korea Institute of Materials Science, Changwon, South Korea
  11. 김양도School of Materials Science and Engineering, Pusan National University, Busan, South Korea
  12. Yang, Sangsun교신저자Powder Technology Department, Korea Institute of Materials Science, Changwon, South Korea

초록

Ternary Bi-Sn-In micropowders and nanoparticles were prepared as a composite solder material via a gas atomization process and a chemical reduction method, respectively. The nanoparticles, with a 71.1 degrees C melting temperature, entered among the intervals of the higher melting temperature (79.4 degrees C) micropowders, and then reflowed at 110. C on a flexible polyethylene terephthalate (PET) substrate. This considerably increased the thermal diffusivity of the nanoparticles to refine the surface morphology of the solder bumps. Their adhesion strength also increased from an average shear force of 0.33-0.43 N by viscosity improvement, afforded to the reinforcement of 5.0 wt.% added nanoparticles. However, the adhesion strength (0.25 N average shear force) of the composite solder bumps deteriorated at 15.0 wt.% added nanoparticles and resulted in a high electrical resistivity (72.53 +/- 8.54 mu Omega cm) due to the formation of their surface-oxidized phases. (C) 2016 Elsevier B.V. All rights reserved.