An Investigation of the Mechanical Properties of a Weldment of 7% Nickel Alloy Steels
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q3
- 저널
- METALS6(11) · 2016
- 피인용
- Web of Science 15
- JCR IF
- JCR 2015 1.574
- ISSN
- 2075-4701
저자
- 박정열제1저자Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, South Korea
- 이제명Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, South Korea
- 김명현교신저자Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, South Korea
초록
During the last decade, the demand for natural gas has steadily increased for the prevention of environmental pollution. For this reason, many liquefied natural gas (LNG) carriers have been manufactured. Since one of the most important issues in the design of LNG carriers is to guarantee structural safety, the use of low-temperature materials is increasing. Among commonly employed low-temperature materials, nickel steel has many benefits such as good strength and outstanding corrosion resistance. Accordingly, nickel steels are one of the most commonly used low-temperature steels for LNG storage tanks. However, the study of fracture toughness with various welding consumables of 7% nickel alloy steel is insufficient for ensuring the structural safety of LNG storage tanks. Therefore, the aim of this study was to evaluate fracture toughness of several different weldments for 7% nickel alloy steels. The weldment of 7% nickel alloy steel was fabricated by tungsten inert gas (TIG), flux cored arc welding (FCAW), and gas metal arc welding (GMAW). In order to assess the material performance of the weldments at low temperature, fracture toughness such as crack tip opening displacement (CTOD) and the absorbed impact energy of weldments were compared with those of 9% nickel steel weldments.
키워드
liquefied natural gasnickel steelweldmentscrack tip opening displacement