TIG Dressing Effects on Weld Pores and Pore Cracking of Titanium Weldments
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q3
- 저널
- METALS6(10) · 2016
- 피인용
- Web of Science 10
- JCR IF
- JCR 2015 1.574
- ISSN
- 2075-4701
저자
- Yi, Hui-Jun제1저자교신저자Hyundai-Rotem Company, Chang-won, South Korea
- Lee, Yong-JunThe 3rd land system team, Defense Agency for Technology and Quality, Chang-won, South Korea
- 이광오School of Mechanical Engineering, Pusan National University, Busan, South Korea
초록
Weld pores redistribution, the effectiveness of using tungsten inert gas (TIG) dressing to remove weld pores, and changes in the mechanical properties due to the TIG dressing of Ti-3Al-2.5V weldments were studied. Moreover, weld cracks due to pores were investigated. The results show that weld pores less than 300 mu m in size are redistributed or removed via remelting due to TIG dressing. Regardless of the temperature condition, TIG dressing welding showed ductility, and there was a loss of 7% tensile strength of the weldments. Additionally, it was considered that porosity redistribution by TIG dressing was due to fluid flow during the remelting of the weld pool. Weld cracks in titanium weldment create branch cracks around pores that propagate via the intragranular fracture, and oxygen is dispersed around the pores. It is suggested that the pore locations around the LBZ (local brittle zone) and stress concentration due to the pores have significant effects on crack initiation and propagation.
키워드
titanium weldingweld porescracksTIG dressingductilityIN-SITU OBSERVATIONPOROSITYALLOYSMICROSTRUCTUREBEHAVIOR