본문 바로가기

Microstructure of evaporated or sputtered CdTe films in relation to heat treatment

문서 유형
연구출판물 · 학술지 논문
등재
KCISCIEScopus
저널 순위
JCR Q4Scopus Q3
저널
JOURNAL OF CERAMIC PROCESSING RESEARCH17(3) · pp.265 · 2016
피인용
Web of Science 1KCI 0
JCR IF
JCR 2015 0.32
ISSN
1229-9162

저자

  1. 김서한제1저자부산대학교
  2. 조상현부산대학교
  3. 이건환한국기계연구원부설 재료연구소
  4. 박인욱한국생산기술연구원
  5. 송풍근교신저자부산대학교

초록

We prepared 1-mu m-thick CdTe films by thermal evaporation or radio frequency magnetron sputtering. The film deposition was conducted at various substrate temperatures (T-s), and sputtered films were post-annealed in air or vacuum. The CdTe films deposited by evaporation had larger grain sizes than the films deposited by sputtering, likely because the bombardment of high-energy particles during sputtering disturbed the crystallization of the film. The sputtered film was amorphous when grown at room temperature (RT), but crystalline when the T-s was increased during deposition. In case of the evaporated films, the preferred orientation was C-(111) when the T-s was at RT. However, when the T-s was increased, the intensity of the X-ray diffraction peak of C-(111) decreased and that of the C-(220) and C-(311) peaks increased. Finally, sputtered films grown at RT were treated with a post-annealing step at various temperatures. After this treatment, there was no significant difference in the grain size and XRD patterns of the films, likely because the maximum annealing temperature, 400 degrees C, was insufficient to change the microstructure of the film.

키워드

CdTeSputteringThermal evaporationHeat treatmentTHIN-FILMSX-RAYGROWTHNUCLEATIONDEPOSITIONSUBSTRATE

식별자

WoS UID
000378163900025
KCI
ART002327619