Polymeric foams for cryogenic temperature application: Temperature range for non-recovery and brittle-fracture of microstructure
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- COMPOSITE STRUCTURES136 · pp.258 · 2016
- 피인용
- Web of Science 50
- JCR IF
- JCR 2015 3.853
- ISSN
- 0263-8223
저자
- 박성보제1저자Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, South Korea
- 이치승Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, South Korea
- Choi, Sung-WoongLNG and Cryogenic Technology Center, Department of Extreme Energy System, Korea Institute of Machinery and Materials, Gimhae, South Korea
- 김정현Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, South Korea
- Bang, Chang-SeonSystem Research and Development, Cryogenic Research Development Center, Samsung Heavy Industries Co., Ltd, Seongnam, South Korea
- 이제명교신저자Department of Naval Architecture and Ocean Engineering, Pusan National University, Busan, South Korea
초록
In the present study, low-temperature material characteristics of polyurethane foam, glass fiberreinforced polyurethane foam, and polyisocyanurate foam were investigated. These foams are key candidate materials for use in membrane-type liquefied natural gas insulation systems. Liquefied natural gas insulation systems should be able to withstand severe environmental conditions, such as fluid induced impact loading under cryogenic temperatures. For the robust design of insulation system, both failure characteristics and deformation recovery capacity of the materials must be evaluated. Therefore, the failure characteristics and the deformation recovery ratio of the foams were investigated at various temperatures and strain rate levels. The present study revealed that the fracture behavior and the recovery ratio were significantly affected by decreases in temperature. As a newly obtained insight, it has been found that the recovery ratio for all tested materials significantly decreased at -163 degrees C. This finding is the opposite of the behavior that typically occurs at low temperatures. In particular, polyurethane foam specimen after experiment at the temperature of -163 degrees C was easily broken into pieces even under the application of small loads. In addition, it has been revealed that polyisocyanurate foam showed superior mechanical characteristics at cryogenic temperatures owing to the ring structure of isocyanurate. (C) 2015 Elsevier Ltd. All rights reserved.
키워드
Polyurethane foamGlass fiber-reinforced polyurethane foamPolyisocyanurate foamCryogenic temperatureCompressive failureStress-strain relationshipRIGID POLYURETHANE FOAMSTRAIN-RATEMECHANICAL-BEHAVIORDENSITYREINFORCEMENT