Measurement of friction factor of nickel foam anode at high temperature condition of carbonate flow in direct coal fuel cell system
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- APPLIED THERMAL ENGINEERING89 · pp.600 · 2015
- 피인용
- Web of Science 5
- JCR IF
- JCR 2014 2.739
- ISSN
- 1359-4311
저자
- 김학덕제1저자School of Mechanical Engineering, Pusan National University, South Korea
- 김강욱School of Mechanical Engineering, Pusan National University, South Korea
- 송은혜School of Mechanical Engineering, Pusan National University, South Korea
- 송주헌교신저자School of Mechanical Engineering, Pusan National University, South Korea
초록
In this study, the high-temperature hydraulic characteristics of an actual molten carbonate mixture flow through a porous nickel foam were examined. The velocity and head loss were measured at the high-temperature and flow conditions used in a practical direct coal fuel cell (DCFC) system. Different pore and tube diameters were used for the nickel foam. The experimental data for the friction factor and Reynolds number were compared at the Darcy flow regime with the classical relationship from the theoretical prediction. Finally, the relative contribution of the tube walls and pores on the head loss (pressure drop) behavior were described. (C) 2015 Elsevier Ltd. All rights reserved.
키워드
DCFCPorous nickel foamFriction factorMolten carbonate flowDarcy flow regimePore effectMETAL FOAMSPRESSURE-DROPLAMINAR-FLOWWALLVISCOSITYFLUID