Preparation and properties of high-performance recyclable ethylene propylene diene rubber
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 저널
- JOURNAL OF APPLIED POLYMER SCIENCE132(44) · 2015
- 피인용
- Web of Science 5
- JCR IF
- JCR 2014 1.768
- ISSN
- 0021-8995
저자
- 김정수제1저자Industrial Materials Fusion Technology Center, Korea Institute of Footwear and Leather Technology, Busan, South Korea
- Bae, Jong-WooIndustrial Materials Fusion Technology Center, Korea Institute of Footwear and Leather Technology, Busan, South Korea
- Lee, Jin-HyokIndustrial Materials Fusion Technology Center, Korea Institute of Footwear and Leather Technology, Busan, South Korea
- 이영희Department of Organic Material Science and Engineering, Pusan National University, Busan, South Korea
- 김한도교신저자Department of Organic Material Science and Engineering, Pusan National University, Busan, South Korea
초록
To obtain high-performance recyclable ethylene propylene diene rubber (EPDM), EPDM was chemically functionalized as follows: EPDM was grafted with citraconic acid (CCA) by radical melt polymerization to produce a grafted EPDM (EPDM-g-CCA), and EPDM-g-CCA was reacted with various amino acids by melt condensation reaction to give amidated copolymers (EPDM-g-CCA-2-Am, EPDM-g-CCA-7-Am, and EPDM-g-CCA-12-Am, where the n indicates the carbon number of amino acid), and then ionomers (EPDM-g-CCA/n-Am/Io) were prepared by melt reaction of EPDM-g-CCA/n-Ams with Zinc oxide (ZnO)/zinc stearate (ZnSt). The mechanical properties/compression set (CS) resistance (elasticity)/recyclability of pristine EPDM, EPDM-g-CCA, EPDM-g-CCA/n-Am, and ionomers sheet samples were compared. The tensile strength/modulus, tear strength, and elasticity of samples were mostly increased in the order of ionomers>EPDM-g-CCA/n-Ams>EPDM-g-CCA>pristine EPDM. The properties of ionomers increased significantly with increasing the carbon number in amino acid up to seven, and then levelled off or decreased a little. The tensile strength/elasticity (compression set resistance) of recyclable ionomer (EPDM-g-CCA/7-Am/Io) was found to be approximate to 9.42/approximate to 2.31 times of pristine EPDM, respectively. (c) 2015 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015, 132, 42718.
키워드
mechanical propertiesrecyclingsynthesis and processingCARBOXYLATED NITRILE RUBBERMALEIC-ANHYDRIDEVISCOELASTIC BEHAVIORCROSS-LINKINGIONOMERSEPDMPOLYPROPYLENECOPOLYMERSPOLYMERSSALTS