Effect of Si, Mn, Sn on Tensile and Corrosion Properties of Mg-4Zn-0.5Ca Alloys for Biodegradable Implant Materials

문서 유형
연구출판물 · 학술지 논문
등재
KCISCIEScopus
저널 순위
JCR Q1Scopus Q2
저널
Korean Journal of Metals and Materials53(3) · pp.220 · 2015
피인용
Web of Science 9KCI 4
JCR IF
JCR 2014 1.405
ISSN
1738-8228

저자

  1. 조대현제1저자부산대학교 재료공학과
  2. 남지훈부산대학교 재료공학과
  3. 이병우부산대학교
  4. 박지영부산대학교 재료공학과
  5. 신현정부산대학교 재료공학과
  6. 박익민교신저자부산대학교

초록

Effect of elements Si, Mn, Sn on tensile and corrosion properties of Mg-4Zn-0.5Ca alloys were investigated. The results of tensile properties show that the yield strength, ultimate tensile strength and elongation of Mg-4Zn-0.5Ca alloy increased significantly with the addition of 0.6 wt% Mn. This is considered the grain refinement effect due to addition of Mn. However addition of 0.6 wt% Si decreased yield strength, ultimate tensile strength and elongation. The bio-corrosion behavior of Mg-4Zn-0.5Ca-X alloys were investigated using immersion tests and potentiodynamic polarization test in Hank's solution. Immersion test showed that corrosion rate of Mg-4Zn-0.5Ca-0.6Mn alloy was the lowest rate and addition of 1.0 wt% Sn accelerated corrosion rate due to micro-galvanic effect in alpha-Mg/CaMgSn phases interface. And corrosion potential (E-corr) of Mg-4Zn-0.5Ca-0.6Mn alloy was the most noble among Mg-4Zn-0.5Ca-X alloys.

키워드

biomaterialscastingcorrosionscanning electron microscopy (SEM)magnesium alloyAS-CASTMECHANICAL-PROPERTIESCREEP-PROPERTIESMICROSTRUCTUREMAGNESIUMBIOMATERIALSSR