Effects of thermal aging on the microstructure of Type-II boundaries in dissimilar metal weld joints
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- JOURNAL OF NUCLEAR MATERIALS459 · pp.5 · 2015
- 피인용
- Web of Science 46
- JCR IF
- JCR 2014 1.865
- ISSN
- 0022-3115
저자
- Yoo, Seung Chang제1저자School of Mechanical and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Eonyang-eup, Ulju-gun, Ulsan, South Korea
- Choi, Kyoung JoonSchool of Mechanical and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Eonyang-eup, Ulju-gun, Ulsan, South Korea
- 반치범School of Mechanical Engineering, Pusan National University, Geumjeong-Gu, Pusan, South Korea
- Kim, Si HoonSchool of Mechanical and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Eonyang-eup, Ulju-gun, Ulsan, South Korea
- Kim, Ju YoungSchool of Mechanical and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Eonyang-eup, Ulju-gun, Ulsan, South Korea
- Kim, Ji Hyun교신저자School of Mechanical and Nuclear Engineering, Ulsan National Institute of Science and Technology (UNIST), Eonyang-eup, Ulju-gun, Ulsan, South Korea
초록
In order to investigate the effects of long-term thermal aging on the microstructural evolution of Type-II boundary regions in the weld metal of Alloy 152, a representative dissimilar metal weld was fabricated from Alloy 690, Alloy 152, and A533 Gr.B. This mock-up was thermally aged at 450 degrees C to accelerate the effects of thermal aging in a nuclear power plant operation condition (320 degrees C). The microstructure of the Type-ll boundary region of the weld root, which is parallel to and within 100 mu m of the fusion boundary and known to be more susceptible to material degradation, was then characterized after different aging times using a scanning electron microscope equipped with an energy dispersive X-ray spectroscope for micro-compositional analysis, electron backscattered diffraction detector for grain and grain boundary orientation analysis, and a nanoindenter for measurement of mechanical properties. Through this, it was found that a steep compositional gradient and high grain average misorientation is created in the narrow zone between the Type-II and fusion boundaries, while the concentration of chromium and number of low-angle grain boundaries increases with aging time. A high average hardness was also observed in the same region of the dissimilar metal welds, with hardness peaking with thermal aging simulating an operational time of 15 years. (C) 2015 Elsevier B.V. All rights reserved.
키워드
STRESS-CORROSION CRACKINGENVIRONMENTALLY-ASSISTED CRACKINGHIGH-TEMPERATURE WATERHEAT-AFFECTED ZONEALLOYINTERFACESREGIONCHEMISTRYREACTORBEHAVIOR