Effect of thermal annealing on the structural, electrical and optical properties of Al-Ni co-doped ZnO thin films prepared using a sol-gel method
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 저널
- SURFACE & COATINGS TECHNOLOGY261 · pp.149 · 2015
- 피인용
- Web of Science 32
- JCR IF
- JCR 2014 1.998
- ISSN
- 0257-8972
저자
- Zhang, X. L.제1저자School of Materials Science and Engineering, Pusan National University, Geumjeong-gu, Busan, South Korea
- Hui, K. S.교신저자Department of Mechanical Convergence Engineering, Hanyang University, Seongdong-gu, Seoul, South Korea
- Bin, FengState Key Laboratory of High-Temperature Gas Dynamics, Institute of Mechanics, Chinese Academy of Science, Beijing, China
- 후이School of Materials Science and Engineering, Pusan National University, Geumjeong-gu, Busan, South Korea
- Li, LeiSchool of Materials Science and Engineering, Pusan National University, Geumjeong-gu, Busan, South Korea
- 조영래School of Materials Science and Engineering, Pusan National University, Geumjeong-gu, Busan, South Korea
- 라자람 사카람 마네Centre for Nano-materials and Energy Devices, School of Physical Sciences, SRTM University, Nanded, India
- Zhou, WeiDepartment of Mechanical and Electrical Engineering, Xiamen University, Xiamen, China
초록
Al-Ni co-doped ZnO (NiAl:ZnO) thin films were deposited on glass substrates using a sol-gel method. Based on a previous study, Zn-1 (-) xAlxO (AZO; Al/Zn = 1.5 mol%) thin films optimized with a Ni content of 0.5 mol% were annealed at different temperatures from 450 to 600 degrees C in N-2/H-2 (95/5) forming gas for 1 h. The effects of the annealing temperature on the structural, electrical and optical properties were determined. X-ray diffraction showed that NiAl:ZnO thin film annealed at 500 degrees C exhibited the best crystallization quality. XPS revealed the presence of metallic Ni and Ni2O3 states, as well as Ni and Al atoms were successfully doped in NiAl:ZnO films, which did not result in a change in ZnO crystal structure and orientation. Scanning electron microscopy showed that the films were smooth and compact, and the grain size increased with increasing annealing temperature from similar to 23.8 nm to similar to 34.6 nm. According to the Hall Effect measurements, when the temperature reached 500 degrees C the resistivity of the thin film showed the lowest value of 1.05 x 10(-3) (Omega cm), which is the lowest resistivity reported for NiAl:ZnO films. The UV-Vis transmission spectra showed a high transmittance of more than 80% in the visible light range, and the band gap of the films was increased from 3.30 to 3.55 eV. This study showed that the annealing temperature in the forming gas is a vital factor affecting the quality of thin films. In addition, 500 degrees C was found to be the most appropriate annealing temperature for NiAl:ZnO films. This study provides a simple and efficient method for preparing high quality, high transparency and low resistivity NiAl:ZnO films for optoelectronic applications. (C) 2014 Elsevier B.V. All rights reserved.
키워드
Al-Ni co-doped ZnOAnnealing temperatureSol-gel methodForming gasTEMPERATURENANORODSNANOSTRUCTURESNANOPLATELETSADSORPTIONSURFACESXPS