본문 바로가기

Characterization of 1,2,3-triazole crosslinked polymers based on azide chain-ends prepolymers and a dipolarophile curing agent as propellant binders: The effect of a plasticizer

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q1Scopus Q1
피인용
Web of Science 19
JCR IF
JCR 2013 2.637
ISSN
1876-1070

저자

  1. 이동훈제1저자Department of Chemical Engineering, Pusan National University, Busan, South Korea
  2. Kim, Kyoung TaeDepartment of Chemistry, Kwangwoon University, Seoul, South Korea
  3. 정해지Department of Polymer Science and Engineering, Pusan National University, Busan, South Korea
  4. Kim, Sang HyunDepartment of Chemistry, Kwangwoon University, Seoul, South Korea
  5. Park, SangjoonDepartment of Chemistry, Kwangwoon University, Seoul, South Korea
  6. Jeon, Heung BaeDepartment of Chemistry, Kwangwoon University, Seoul, South Korea
  7. 백현종Department of Polymer Science and Engineering, Pusan National University, Busan, South Korea
  8. Min, Byoung SunAdvanced Propulsion Technology Center, Agency for Defense Development, Daejeon, South Korea
  9. 김원호교신저자Department of Chemical Engineering, Pusan National University, Busan, South Korea

초록

The 1,2,3-triazole crosslinked polymers with potential use as a binder system in solid rocket propellants were prepared by mixing of an azide chain-ends diazide prepolymer, a dipolarophile curing agent, which act as a crosslinker, and a plasticizer at C C/N-3 ratio of 1.1. A wide range of the plasticizer ratios were investigated: 0-300 wt% for the polycaprolactone (PCP) and polycaprolactone ether (PCE) prepolymer based binders, and 0-500 wt% for the polyethylene glycol (PEG) prepolymer based binder. Even at high amounts of plasticizer, sufficient initial reactivity and good conversion were obtained, however the increase of viscosity was considerably delayed. Crystalline domains of in the 1,2,3-triazole crosslinked polymers were effectively eliminated by the plasticizer. The tensile strength and modulus (100% and 300%, respectively) decreased with increasing of the amount of plasticizer whereas the elongation at the break was only modestly affected. PCP showed excellent elongation at the break compared to PEG at the same levels of plasticizer as well as good tensile strength. In contrast, the binder network prepared from the PCE prepolymer collapsed due to its low degree of crosslinking. (C) 2014 Taiwan Institute of Chemical Engineers. Published by Elsevier B.V. All rights reserved.

키워드

1,2,3-Triazole crosslinked polymersAzide chain-ends prepolymerDipolarophile curing agentPlasticizerThermal propertiesMechanical propertiesTRIAZOLE-OLIGOMERSCYCLOADDITION

식별자

WoS UID
000347742300036