Thermoelectric generator based on a bismuth-telluride alloy fabricated by addition of ethylene glycol
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q2Scopus Q1
- 저널
- CURRENT APPLIED PHYSICS14(12) · pp.1788 · 2014
- 피인용
- Web of Science 15KCI 0
- JCR IF
- JCR 2013 2.026
- ISSN
- 1567-1739
저자
초록
This paper introduces a new method to selectively fabricate n-type and p-type bismuth (Bi)-telluride (Te) thermoelectric materials by the rate of addition of ethylene glycol (EG) in the Bi-Te co-electrodeposition solution. As the amount of added EG is increased, the atomic ratio of Bi in the deposited Bi-Te alloy reached a slope of 0.463 (at.% of Bi/vol.% of EG), and increased in a linear manner. When the EG content reached approximately 20% v/v, the n-type material changed into a p-type. This change implies that adjusting the EG content in the electrodeposition solution affords simple control of the Bi-Te composition. To demonstrate the applicability of the developed thermoelectric materials, thermoelectric generators (TEGs) were fabricated using electrodeposited n-type (using solution without EG) and p-type (using solution with 30% v/v EG) Bi-Te alloys. The Seebeck voltage of the pair of n-type and p-type thermoelectric materials was 140 mV and the power generated from the pair was 24.36 nW at a 10 degrees C temperature difference. (C) 2014 Elsevier B.V. All rights reserved.
키워드
Thermoelectric generatorBismuth telluride alloyPulse electrodepositionEthylene glycolELECTROCHEMICAL DEPOSITIONFILMSBI2TE3ELECTRODEPOSITIONSB2TE3
식별자
- WoS UID
- 000345397900033
- KCI
- ART001938798



로그인
연구물 목록으로