본문 바로가기

Preparation and Properties of UV-Curable Fluorinated Polyurethane Acrylates

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q2
피인용
Web of Science 42
JCR IF
JCR 2013 1.64
ISSN
0021-8995

저자

  1. 박정민제1저자Department of Organic Material Science and Engineering, Pusan National University, South Korea
  2. 이영희Department of Organic Material Science and Engineering, Pusan National University, South Korea
  3. 박현Global Core Research Center for Ships and Offshore Plants, Pusan National University, South Korea
  4. 김한도교신저자Department of Organic Material Science and Engineering, Pusan National University, South Korea

초록

A series of UV-curable polyurethane acrylates (PUA0, FPUA3, FPUA6, FPUA 9 FPUA12, FPUA15, where the numbers indicate the wt % of perfluoroalkyl acrylate), were prepared from a reactive oligomer [4,4 '-dicyclohexymethanediisocyanate(H12MDI)/ poly(tetramethylene glycol)(PTMG)/2-hydroxyethyl methacrylate (HEMA): 2/1/2 molar ratio, prepolymer:40 wt %] and diluents [methyl methacrylate (MMA, 20 wt %)/ isobornyl acrylate (IBOA, 40-25 wt %)/heptadecafluorodecyl methacrylate (PFA, 0-15 wt), total diluents: 60 wt %]. This study examined the effect of PFA/IBOA weight ratio on the properties of the UV-curable polyurethane acrylates for antifouling coating materials. The as-prepared UV-curable coating material containing a 15 wt % PFA content in diluents (MMA/IBOA/PFA) form a heterogeneous mixture, indicating that a PFA content of approximately 15 wt % was beyond the limit of the dilution capacity of diluents for the oligomer. In the wavelength range of 400-800 nm, the UV-cured PUA0 film sample was quite transparent (transmittance%: near 100%). On the other hand, the transmittance% of the FPUA film sample decreased markedly with increasing PFA content. XPS showed that the film-air surface of the UV-cured polyurethane acrylate film had a higher fluorine content than the film-glass dish interface. As the PFA content increased from 0 to 12 wt %, the surface tension of the UV-cured urethane acrylates decreased from 26.8 to 15.6 mN/m, whereas the water/methylene iodide contact angles of the film-air surface increased from 90.1/63.6 degrees to 120.9/87.1 degrees. These results suggest that the UV-curable polyurethane acrylates containing a PFA content up to 12 wt % have strong potential as fouling-release coating materials. (c) 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014, 131, 40603.

키워드

coatingspolyurethanesproperties and characterizationsurfaces and interfacesBLOCK-COPOLYMERSSURFACE SEGREGATIONWETTING PROPERTIESSIDE-CHAINSPOLYMERSDISPERSIONEMULSIONSCOATINGSTENSION

식별자

WoS UID
000336453600009