Effect of the Tempered Martensite Matrix and Granular Bainite on Stretch-Flangeability for 980 MPa Hot-Rolled Steel

문서 유형
연구출판물 · 학술지 논문
등재
KCISCIEScopus
저널 순위
JCR Q2Scopus Q1
저널
Korean Journal of Metals and Materials52(2) · pp.113 · 2014
피인용
Web of Science 14KCI 9
JCR IF
JCR 2013 1.022
ISSN
1738-8228

저자

  1. 이주승부산대학교
  2. 이명진부산대학교
  3. 도형협현대제철
  4. 김성주현대제철
  5. 강남현교신저자부산대학교

초록

The main goal of the study is to obtain high strength and formability for automotive sheet steels such as wheel and chassis. Ferrite-based steels developed previously exhibited superior stretch-flangeability to 780 MPa and even to 980 MPa grade steels. However, it was difficult to achieve 980 MPa tensile strength sufficiently. To achieve a superior stretch-flangeability and to acquire a sufficiently high strength over 980 MPa, a composition of Fe-Cr-Ti-B was developed for hot rolling. The manufactured steel was coiled for 1 hour at 430, 450, and 470 degrees C. Specifically, 998 MPa ultimate tensile strength, 11% total elongation, and a 59% excellent hole expansion ratio were obtained by microstructural constituents of a tempered martensite matrix and granular bainite when the coiling was conducted at 470 degrees C. As the coiling temperature varied from 470 to 430 degrees C, the fraction of granular bainite decreased and that of tempered martensite increased. Therefore, the deviation of phase fractions between two phases decreased at 470 degrees C coiling. Furthermore, as the hole expansion ratio (HER) increased, the hardness deviation of the two phases decreased. As the HER value increased, the crack propagation path dispersed on the second fracture surface and fracture was significantly delayed. Therefore, hot rolled steels using a tempered martensite matrix and granular bainite had the same behavior of stretch-flangeability with respect to the hardness deviation and crack propagation path as compared with the steels using a ferrite matrix. For high strength steels composed of the tempered martensite matrix and granular bainite, however, the minimal deviation between the two constituent phases was acknowledged as an important factor to increase stretch-flangeability.

키워드

metalsrollingmicrostructureprecipitationhardness teststretch-flangeabilityHOLE-EXPANSION-RATIOMECHANICAL-PROPERTIESLOW-CARBONSTRENGTHFORMABILITYSHEETSMICROSTRUCTURETEMPERATUREBEHAVIOR

식별자

WoS UID
000331346900003
KCI
ART001849044