본문 바로가기

Effect of Indium Content on the Melting Point, Dross, and Oxidation Characteristics of Sn-2Ag-3Bi-xIn Solders

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q2
피인용
Web of Science 12
JCR IF
JCR 2012 0.934
ISSN
1043-7398

저자

  1. 전애정제1저자National Core Research Center (NCRC), Pusan National University, South Korea
  2. Kim, Seong-JunSamsung Electronics Co., Ltd., South Korea
  3. Lee, Sang-HoonKorea Institute of Materials Science, South Korea
  4. 강정윤교신저자National Core Research Center (NCRC), Pusan National University, South Korea

초록

This paper presents the effect of indium (In) content on the melting temperature, wettabililty, dross formation, and oxidation characteristics of the Sn-2Ag-3Bi-xIn alloy. The melting temperature of the Sn-2Ag-3Bi-xIn alloy (2 <= x <= 6) was lower than 473 K. The melting range between the solidus and liquidus temperatures was approximately 20 K, irrespective of the indium content. As the indium content increased, the wetting time increased slightly and the maximum wetting force remained to be mostly constant. The dross formation decreased to approximately 50% when adding 1In to Sn-2Ag-3Bi, and no dross formation was observed in the case of Sn-2Ag-3Bi-xIn alloy (x >= 1.5) at 523K for 180 min. Upon approaching the inside of the oxidized solder of the Sn-2Ag-3Bi-1.5In alloy from the surface, the O and In contents decreased and the Sn content increased based on depth profiling analysis using Auger electron spectroscopy (AES). The mechanism for restraining dross (Sn oxidation) of Sn-2Ag-3Bi alloy with addition of indium may be due to surface segregation of indium. This is due to the lower formation energy of indium oxide than those of Sn oxidation.

키워드

Sn-Ag-Bi-In alloywettabilitydrossoxidationLEAD-FREE SOLDERSN-AG-CUMECHANICAL-PROPERTIESTENSILE PROPERTIESBIMICROSTRUCTUREALLOYSTEMPERATURERELIABILITYEVOLUTION