Mechanical Properties and Molecular Structure of Rubber Materials with Different Hardnesses for Vibration Isolation of Elevator Cabins

문서 유형
연구출판물 · 학술지 논문
등재
KCISCIEScopus
저널 순위
JCR Q1Scopus Q1
저널
Korean Journal of Metals and Materials51(10) · pp.713 · 2013
피인용
Web of Science 7KCI 0
JCR IF
JCR 2012 1.201
ISSN
1738-8228

저자

  1. 신병길Pusan National University
  2. 윤상현Pusan National University
  3. 이희수부산대학교
  4. 구영석부산대학교
  5. 정영근부산대학교
  6. Ingoo Kang교신저자Korea Testing Laboratory

초록

The mechanical properties and molecular structure of rubber materials for reducing the vibration of elevator cabins were studied with respect to the hardnesses change to confirm the degradation behavior by temperature (85 degrees C) and humidity (85% R.H.). To examine the effects of hardness on the mechanical properties after thermal and hydrothermal aging, the international rubber hardness degree (IRHD), tensile strength, and elongation % were compared with the elastic modulus as a function of degradation time. The microstructure showed that the crack growth of the rubber material with high hardness was fast after hydrothermal aging. It originated from a C = C bonding decrease, and the C = O and C-O-C bonding were increased by the penetration of humidity. In the results of solid-state C-13 nuclear magnetic resonance (NMR) spectroscopy to confirm the molecular structure, several peaks were assigned to respective vulcanized structures along with mechanical properties. Therefore, the degradation behavior after thermal/hydrothermal aging was different according to low/high hardness: The mechanical properties of the rubber material with high hardness rapidly decreased due to the high density of cross-links and chain scission.

키워드

rubber materialsinternational rubber hardness degreemechanical propertiessolid state C-13 NMRpolymer structureSTATE C-13 NMRNATURAL-RUBBERLIFE PREDICTIONFT-IRDEGRADATIONSPECTROSCOPYVULCANIZATIONMORPHOLOGYCOMPONENTCOMPOUND