Crystal Growth and Photoluminescence Properties of Sm3+ Doped CeO2 Nanophosphors by Solvothermal Method

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
Scopus Q2
저널
JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY13(9) · pp.6060 · 2013
피인용
Web of Science 3
JCR IF
JCR 2012 1.149
ISSN
1533-4880

저자

  1. Yang, Hyun Kyoung제1저자Jeju Global Res Ctr, Korea Inst Energy Res, KO
  2. Moon, Byung Kee부경대학교, Dept Phys, KO
  3. Choi, Byung Chun부경대학교, Dept Phys, KO
  4. Jeong, Jung Hyun교신저자부경대학교, Dept Phys, KO
  5. 김광호부산대학교, 공과대학, 재료공학부, 무기재료공학전공, KO

초록

The phosphor of CeO2 activated with the trivalent rare-earth Sm3+ ions were synthesized by using a solvothermal method. The CeO2:Sm3+ powders were finally obtained through calcination process sintered in the air at 800-1200 degrees C. The synthesized phosphors were characterized systematically by X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), photoluminescence (PL) and photoluminescence excitation spectra (PLE). The XRD and FE-SEM results reveal that the phosphor exhibit agglomerated spherical shape and with the increase of sintering temperature peaks become sharper and narrower and the crystal sizes also increase, respectively. The room temperature photoluminescence spectra of Sm3+ doped CeO2 powders were recorded on a PTI (Photon Technology International) flurimeter using a Xe-arc lamp with a power of 60 W. The emitted radiation was dominated by the orange light with the characteristic emission of Sm3+ from the transitions of (4)G(5/2) -> H-6(5/2),(7/2). The sharp emission properties show that the CeO2 has the potential to serve as a host material for rare-earth doped laser crystal and phosphor material.