Effect of wear debris of Al2O3, ZrO2 and WC balls on Y-alpha/beta-SiAlON ceramics consolidated by spark plasma sintering
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- METALS AND MATERIALS INTERNATIONAL19(2) · pp.163 · 2013
- 피인용
- Web of Science 5
- JCR IF
- JCR 2012 1.434
- ISSN
- 1598-9623
저자
- Chun, Sungsu제1저자School of Materials Science and Engineering, Yeungnam University, South Korea
- Min, Bong-KiCenter for Research Facilities, Yeungnam University, South Korea
- Han, Young-HwanSchool of Materials Science and Engineering, Yeungnam University, South Korea
- 김용문NCRC for Hybrid Materials Solution, Pusan National University, South Korea
- 이경석NCRC for Hybrid Materials Solution, Pusan National University, South Korea
- 정영근NCRC for Hybrid Materials Solution, Pusan National University, South Korea
- 김광호NCRC for Hybrid Materials Solution, Pusan National University, South Korea
- Kim, Young-KiCentral Research Facility, Ulsan National Institute of Science and Technology, South Korea
- Kim, Sukyoung교신저자School of Materials Science and Engineering, Yeungnam University, South Korea
초록
Three types of Y-alpha/beta-SiAlON powders were prepared by mixing and milling the raw materials for 20 h using Al2O3, ZrO2, and WC balls, thereafter denoted as SNA, SNZ and SNW, respectively. The three types of specimens were sintered using spark plasma sintering (SPS) at 1510 A degrees C for 5 min under 30 MPa in a vacuum. alpha-phases (SiAlON and Si3N4) and beta-SiAlON phase were observed in the SNA and SNZ specimens, but only the beta-SiAlON phase existed in the SNW specimen. The wear debris of the WC balls affected the grain boundary properties and eventually promoted the full phase transformation of alpha-Si3N4 into alpha- and beta-SiAlON phases. However, SNA and SNZ were partially transformed into alpha- and beta-SiAlON phases. The Vickers hardness of SNA was the highest (18.7 GPa), due to its having the highest content of alpha-phase, but its fracture toughness was the lowest (4.09 MPam(1/2)) due to its having the lowest content of beta-SiAlON phase. The wear debris and secondary phases existed at the grain boundary, mostly at the triple junction, and also affected the color. The color of the sintered specimen was quite different depending on the milling media.
키워드
wearSiAlONspark plasma sintering (SPS) milling mediafracture toughnessSILICON-NITRIDE CERAMICSADDITIVESFRACTUREPHASE