본문 바로가기

Morphology and dynamic mechanical properties of styrenebutadiene rubber/silica/organoclay nanocomposites manufactured by a latex method

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2Scopus Q1
저널
JOURNAL OF APPLIED POLYMER SCIENCE128(4) · pp.2344 · 2013
피인용
Web of Science 12
JCR IF
JCR 2012 1.395
ISSN
0021-8995

저자

  1. Kim, Wook-Soo제1저자Research and Development Division, NEXEN TIRE Corporation, South Korea
  2. Jang, Suk HeeResearch and Development Division, NEXEN TIRE Corporation, South Korea
  3. Kang, Yong GuResearch and Development Division, NEXEN TIRE Corporation, South Korea
  4. Han, Min HyunResearch and Development Division, NEXEN TIRE Corporation, South Korea
  5. 현규Department of Chemical Engineering, Pusan National University, South Korea
  6. 김원호교신저자Department of Chemical Engineering, Pusan National University, South Korea

초록

In this study, the styrenebutadiene rubber (SBR)/N, N-dimethyldodecylamine-montmorillonite nanocomposite was prepared with a latex method by applying DDA to Na+-MMT as a modifier. The dispersion of silica and the dynamic viscoelastic properties of the SBR/silica (60 phr) compound were studied by replacing 7 phr of the silica with organoclay. By the analysis of transmission electron microscopy images and the Payne effect, the dispersion of silica in the SBR/silica (53 phr)/DDA-MMT (7 phr) compound was further improved as compared to the SBR/silica (60 phr) compound that used only silica as a filler. The Payne effect curve of the SBR/silica/DDA-MMT compound was close to the curve of the SBR/silica (53 phr) compound. This indicates that organically modified silicate did not form fillerfiller networks with silica. Also, the SBR/DDA-MMT compound filled with silica showed the highest values of Tg and tan at 0 degrees C. This result was attributed to the shift of the tan curve to the right because of the relatively higher degree of crosslink. Consequently, the SBR/silica/organoclay nanocomposite showed the best skid resistance due to the increase of Tg, and the best rolling resistance due to the reduced fillerfiller networks. High 100% and 300% modulus values were also achieved. (c) 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013

키워드

SBR latexorganoclaysilicadual filler systemdynamic viscoelastic propertiesRUBBER/ORGANOCLAY NANOCOMPOSITESFILLERSILICARUBBER

식별자

WoS UID
000315217400015