Effect of Energy Density on Low-Shrinkage Composite Resins: Diode-Pumped Solid State Laser Versus Quartz-Tungsten-Halogen Light-Curing Unit
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q2Scopus Q2
- 저널
- PHOTOMEDICINE AND LASER SURGERY31(1) · pp.28 · 2013
- 피인용
- Web of Science 10
- JCR IF
- JCR 2012 1.634
- ISSN
- 1549-5418
저자
- 허영준제1저자Department of Dental Materials, School of Dentistry and Medical Research Institute, Pusan National University, South Korea
- 이근호Department of Dental Materials, School of Dentistry and Medical Research Institute, Pusan National University, South Korea
- 박정길Department of Conservative Dentistry, School of Dentistry, South Korea
- 노정훈Department of Biomedical Engineering, School of Medicine, South Korea
- García-Godoy, FranklinCollege of Dentistry, University of Tennessee Health Science Center, United States
- 김형일Department of Dental Materials, School of Dentistry and Medical Research Institute, Pusan National University, South Korea
- 권용훈교신저자Department of Dental Materials, School of Dentistry and Medical Research Institute, Pusan National University, South Korea
초록
Objective: The purpose of the present study was to evaluate the effect of energy density on the polymerization of low-shrinkage composite resins. Background data: The number of photons needs to initiate the polymerization process can be controlled by light intensity and curing time through the form of energy density. Materials and methods: For the study, two methacrylate-based (Premise [PR] and Venus Diamond [VE]) and one silorane-based (Filtek LS [LS]) composite resins were light cured using a quartz-tungsten-halogen (QTH) light-curing unit (LCU) and a 473nm diode-pumped solid state (DPSS) laser. Degree of conversion (DC), microhardness, refractive index, and polymerization shrinkage were evaluated under different energy densities. Through the study, the feasibility of DPSS laser as a light source was tested as well. Results: LS showed the highest DC and refractive index both on the top and bottom surfaces, and the least polymerization shrinkage among the tested specimens. For the same or similar energy density, QTH and DPSS showed insignificant DC difference (p > 0.05). On the other hand, for microhardness, except for one case at the bottom surface, QTH and DPSS showed significant difference (p < 0.001). DPSS generated slightly lower polymerization shrinkage than that by QTH. Conclusions: DC, microhardness, refractive index, and polymerization shrinkage were linearly correlated with energy density. In most cases, there was a strong linear correlation among DC, mirohardness, and refractive index. The DPSS laser of 473nm could polymerize low-shrinkage composite resins to the level that was achieved by the conventional QTH unit.
키워드
DENTAL COMPOSITESPOLYMERIZATION SHRINKAGEPHYSICAL-PROPERTIESMONOMERSPHOTOPOLYMERIZATIONNANOTECHNOLOGYMICROHARDNESSCONTRACTIONOXYGENDEPTH