Crack propagation behavior of TiN coatings by laser thermal shock experiments
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- APPLIED SURFACE SCIENCE258(22) · pp.8752 · 2012
- 피인용
- Web of Science 29
- JCR IF
- JCR 2011 2.103
- ISSN
- 0169-4332
저자
- 최용규제1저자School of Materials Science and Engineering, Pusan National University, South Korea
- 전설School of Materials Science and Engineering, Pusan National University, South Korea
- Jeon, Min-SeokMaterial Testing Center, Korea Testing Laboratory, South Korea
- Shin, Hyun-GyooMaterial Testing Center, Korea Testing Laboratory, South Korea
- 전호환Department of Naval Architecture and Ocean Engineering, Pusan National University, South Korea
- Lee, Youn-SeoungDepartment of Information Communication Engineering, Hanbat National University, South Korea
- 이희수교신저자School of Materials Science and Engineering, Pusan National University, South Korea
초록
The crack propagation behavior of TiN coatings, deposited onto 304 stainless steel substrates by arc ion plating technique, related to a laser thermal shock experiment has been investigated using focused ion beam (FIB) and transmission electron microscopy (TEM). The ablated regions of TiN coatings by laser ablation system have been investigated under various conditions of pulse energies and number of laser pulses. The intercolumnar cracks were predominant cracking mode following laser thermal shock tests and the cracks initiated at coating surface and propagated in a direction perpendicular to the substrate under low loads conditions. Over and above those cracks, the cracks originated from coating-substrate interface began to appear with increasing laser pulse energy. The cracks from the interface also spread out transversely through the weak region of the columnar grains by repetitive laser shock. (C) 2012 Elsevier B. V. All rights reserved.
키워드
Crack propagationLaser ablationFocused ion beamTransmission electron microscopyION-BEAM MILLERCONTACT DEFORMATION(TI,AL)N COATINGSHARD COATINGSFILMSNANOINDENTATIONSTEEL