본문 바로가기

Synthesis and characterization of novel crosslinkable poly(propylenedioxythiophene) derivative as a buffer layer for organic light-emitting diode applications

문서 유형
연구출판물 · 학술지 논문
등재
KCISCIEScopus
저널 순위
JCR Q3Scopus Q2
저널
MACROMOLECULAR RESEARCH20(5) · pp.459 · 2012
피인용
Web of Science 12KCI 2
JCR IF
JCR 2011 1.153
ISSN
1598-5032

저자

  1. 안성광부산대학교
  2. 진성호교신저자부산대학교
  3. 반태원부산대학교
  4. Pachagounder Sakthivel부산대학교
  5. 제갈영순Kyungil University
  6. 이준희동아대학교

초록

A new crosslinkable polythiophene derivative, poly(hexynyl(2)-PDOT-co-heptyl(2)-PDOT), with propylenedioxythiophene moiety containing solubilizing and crosslinkable substitutents as a pendant group were synthesized by oxidative polymerization using FeCl3. The resulting copolymer was soluble in organic solvents and spun cast onto the indium tin oxide-coated glass substrate to create a uniform thin film. After thermal crosslinking and rinsing of the crosslinked thin film using chloroform, the pi-pi transition peak and the absorption edge appeared at almost the same wavelength as that of the untreated copolymer. We fabricated organic light-emitting diodes (OLEDs) in ITO/buffer layer/poly[2-(2'-ethylhexyloxy)-5-methoxy-1,4-phenylenevinylene] (MEH-PPV)/LiF/Ca/Al configuration using either poly(3,4-ethylenedioxythiophene) doped with poly(styrenesulfonate) (PEDOT:PSS) or poly(hexynyl(2)-PDOT-co-heptyl(2)-PDOT) as buffer layers. Due to the intrinsic conductivity of poly(hexynyl(2)-PDOT-co-heptyl(2)-PDOT) vs. that of PEDOT:PSS caused decreased OLED performance. The turn-on voltage of the OLED using poly(hexynyl(2)-PDOT-co-heptyl(2)-PDOT) buffer layer was observed at 5 V. The maximum brightness and luminance efficiencies were 2,597 cd/m(2) at 12 V and 0.3 cd/A, respectively.

키워드

organic light-emitting diode (OLED)buffer layerPEDOT:PDDPPDOTthermal crosslinkingPOLYMERS

식별자

WoS UID
000303538700004
KCI
ART001661717