Crystallization characteristics of La2O3-containing glasses for glass ionomer cement
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- MATERIALS LETTERS72 · pp.137 · 2012
- 피인용
- Web of Science 11
- JCR IF
- JCR 2011 2.307
- ISSN
- 0167-577X
저자
- Abo-Mosallam, H. A.제1저자교신저자Department of Materials Science and Engineering, Pusan National University, South Korea
- 박홍채Department of Materials Science and Engineering, Pusan National University, South Korea
초록
Glasses with general formula 4.5SiO(2)center dot 3Al(2)O(3)center dot 1.5P(2)O(5)center dot(2.5 x)CaO center dot xL(2)O(3)center dot 2.5CaF(2) (x=0.0-1.0) for glass ionomer cement have been prepared by conventional melting and water quenching. The influence of substitution of La2O3 for CaO on glass transition temperature (T-g), setting time and crystallization was studied. An increase in La2O3/CaO ratio shifted T-g to higher temperature. Fluorapatite (Ca-5(PO4)(3)F), mullite (3Al(2)O(3)center dot 2SiO(2)), lanthanum aluminum silicate solid solution, and anorthite (CaO center dot Al2O3 center dot 2SiO(2)) were identified by XRD in the heat-treated materials; then, their formation was dependent on glass composition and heat-treatment temperature. After heat-treating at 750 degrees C with glass samples of La2O3/CaO = 0, 0.25 (molar ratio), only fluorapatite phase was precipitated; however, anorthite was additionally formed at 950 and 1050 degrees C. With further increasing La2O3/CaO ratio and/or heat-treatment temperature, lanthanum aluminum silicate solid solution existed as the major phase. (C) 2011 Elsevier B.V. All rights reserved.
키워드
Amorphous materialsGlass ionomerCrystallizationCementCeramicsCERAMICS
식별자
- WoS UID
- 000301213000041



로그인
연구물 목록으로