Microstructural Effects on Hydrogen Delayed Fracture of 600 MPa and 800 MPa grade Deposited Weld Metal

문서 유형
연구출판물 · 학술지 논문
등재
KCISCIEScopus
저널 순위
JCR Q2Scopus Q1
저널
Korean Journal of Metals and Materials50(1) · pp.52 · 2012
피인용
Web of Science 3KCI 2
JCR IF
JCR 2011 1.007
ISSN
1738-8228

저자

  1. 강희재제1저자부산대학교
  2. 이태우부산대학교
  3. 윤병현포항산업과학연구원
  4. 박서정포항산업과학연구원
  5. 장웅성(재)포항산업과학연구원
  6. 조경목부산대학교
  7. 강남현교신저자부산대학교

초록

Hydrogen-delayed fracture (HDF) was analyzed from the deposited weld metals of 600-MPa and 800-MPa flux-cored arc (FCA) welding wires, and then from the diffusible hydrogen behavior of the weld zone. Two types of deposited weld metal, that is, rutile weld metal and alkali weld metal, were used for each strength level. Constant loading test (CLT) and thermal desorption spectrometry (TDS) analysis were conducted on the hydrogen pre-charged specimens electrochemically for 72 h. The effects of microstructures such as acicular ferrite, grain-boundary ferrite, and low-temperature-transformation phase on the time-to-failure and amount of diffusible hydrogen were analyzed. The fracture time for hydrogen-purged specimens in the constant loading tests decreased as the grain size of acicular ferrite decreased. The major trapping site for diffusible hydrogen was the grain boundary, as determined by calculating the activation energies for hydrogen detrapping. As the strength was increased and alkali weld metal was used, the resistance to HDF decreased.

키워드

ferrous alloysweldingmicrostructurethermal desorption spectrometryhydrogen delayed fractureHIGH-STRENGTH STEELSTHERMAL-ANALYSISLOW-CARBONEMBRITTLEMENTIRONSUSCEPTIBILITYDEGRADATIONFERRITE