Microstructure-Controlled Aerosol-Gel Synthesis of ZnO Quantum Dots Dispersed in SiO2 Nanospheres
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1Scopus Q1
- 저널
- LANGMUIR28(5) · pp.2890 · 2012
- 피인용
- Web of Science 15
- JCR IF
- JCR 2011 4.186
- ISSN
- 0743-7463
저자
- Firmansyah, Dudi Adi제1저자School of Mechanical Engineering, Pusan Clean Coal Center, Pusan National University, South Korea
- Kim, Sang-GyuSchool of Mechanical Engineering, Pusan Clean Coal Center, Pusan National University, South Korea
- 이광승School of Mechanical Engineering, Pusan Clean Coal Center, Pusan National University, South Korea
- Zahaf, RiyanSchool of Mechanical Engineering, Pusan Clean Coal Center, Pusan National University, South Korea
- 김용호School of Mechanical Engineering, Pusan Clean Coal Center, Pusan National University, South Korea
- 이동근교신저자School of Mechanical Engineering, Pusan Clean Coal Center, Pusan National University, South Korea
초록
ZnO quantum dots dispersed in a silica matrix were synthesized from a TEOS:Zn(NO3)(2) solution by a one-step aerosol gel method. It was demonstrated that the molar concentration ratio of Zn to Si (Zn/Si) in the aqueous solution was an efficient parameter with which to control the size, the degree of agglomeration, and the microstructure of ZnO quantum dots (QDs) in the SiO2 matrix. When Zn/Si <= 0.5, unaggregated quantum dots as small as 2 nm were distributed preferentially inside SiO2 spheres. When Zn/Si >= 1.0, however, ZnO QDs of similar to 7 nm were agglomerated and reached the SiO2 surface. When decreasing the ratio of the Zn/Si, a blue shift in the band gap of ZnO was observed from the UV/Visible absorption spectra, representing the quantum size effect. The photoluminescence emission spectra at room temperature denoted two wide peaks of deep-level defect-related emissions at 2.2-2.8 eV. When decreasing Zn/Si, the first peak at similar to 2.3 eV was blue-shifted in keeping with the decrease in the size of the QDs. Interestingly, the second visible peak at 2.8 eV disappeared in the surface-exposed ZnO QDs when Zn/Si >= 1.0.
키워드
SPRAY-PYROLYSISPHOTOLUMINESCENCEPARTICLEOXIDENANOFLUIDSMATRIXLAYERFILMS
식별자
- WoS UID
- 000299864500071



로그인
연구물 목록으로