본문 바로가기

Preparation and Thermal Degradation Behavior of WO(3)-TiO(2) Catalyst for Selective Catalytic Reduction of NOx

문서 유형
연구출판물 · 학술지 논문
등재
KCISCIEScopus
저널 순위
JCR Q4
저널
Korean Journal of Metals and Materials49(8) · pp.596 · 2011
피인용
Web of Science 0KCI 3
ISSN
1738-8228

저자

  1. 신병길제1저자부산대학교
  2. 김장훈부산대학교
  3. 윤상현부산대학교
  4. 이희수부산대학교
  5. 신동우경상대학교
  6. 민화식한국뉴욕주립대학교

초록

Thermal degradation behavior of a WO(3)-TiO(2) monolithic catalyst was investigated in terms of structural, morphological, and physico-chemical analyses. The catalyst with 4 wt.% WO(3) contents were prepared by a wet-impregnation method, and a durability test of the catalysts were performed in a temperature range between 400 degrees C and 800 degrees C for 3 h. An increase of thermal stress decreased the specific surface area, which was caused by grain growth and agglomeration of the catalyst particles. The phase transition from anatase to rutile occurred at around 800 degrees C and a decrease in the Bronsted acid sites was confirmed by structural analysis and physico-chemical analysis. A change in Bronsted acidity can affect to the catalytic efficiency; therefore, the thermal degradation behavior of the WO(3)-TiO(2) catalyst could be explained by the transition to a stable rutile phase of TiO(2) and the decrease of specific surface area in the SCR catalyst.

키워드

porous materialspowder processinggrain growthraman spectroscopycatalytic acid-siteSURFACEVANADIADURABILITYSTABILITYTITANIANH3SCR

식별자

WoS UID
000294277600002
KCI
ART001577295