Synthesis of Ti(3)SiC(2) by infiltration of molten Si
- 문서 유형
- 연구출판물 · 학술지 논문
- 등재
- SCIEScopus
- 저널 순위
- JCR Q1
- 저널
- JOURNAL OF ALLOYS AND COMPOUNDS509(35) · pp.L336 · 2011
- 피인용
- Web of Science 15
- JCR IF
- JCR 2010 2.138
- ISSN
- 0925-8388
저자
- Hwang, Sung Sic제1저자SKC Solmics, South Korea
- Han, JaehoMaterials Science and Technology Division, Korea Institute of Science and Technology, South Korea
- 이동윤교신저자Department of Nanofusion Engineering, College of Nanoscience and Nanotechnology, Pusan National University, South Korea
- Park, Sang-WhanMaterials Science and Technology Division, Korea Institute of Science and Technology, South Korea
초록
High-purity Ti(3)SiC(2) compounds have been fabricated by infiltration of molten Si into a precursor, a partially sintered TiC(x) (x = 0.67) preform. The Si source and the TiC(x) preform were placed side by side on carbon cloth, and the system was heated to 1550 degrees C. Molten Si infiltrated the preform through the carbon cloth, and a direct reaction between TiC(x) and molten Si immediately occurred at the reaction temperature to yield pure Ti(3)SiC(2). We could observe phase formation and the microstructure of the bulk products with time, which were investigated by X-ray diffraction (XRD) and scanning electron microscopy (SEM) equipped with energy-dispersive spectroscopy (EDS). Pure Ti(3)SiC(2) compounds were formed on the exterior of the TiC(x) preform at 1550 degrees C when the sintered TiC(x):Si ingot molar ratio was 3:1.4. At 1550 degrees C, no other minor phases were detected for any of the sintering time ranges. (C) 2011 Elsevier B.V. All rights reserved.
키워드
Ti(3)SiC(2)InfiltrationTiC(x) preformMolten SiHIGH-PURITY TI3SIC2POWDER BLENDTITEMPERATURETI/SI/CAL