Effect of Annealing Ti Foil on The Structural Properties of Anodic TiO2 Nanotube Arrays
- 문서 유형
- 연구출판물 · 학술대회 발표논문
- 등재
- KCISCIEScopus
- 저널 순위
- JCR Q4
- 저널
- JOURNAL OF THE KOREAN PHYSICAL SOCIETY58(3) · pp.575 · 2011
- 피인용
- Web of Science 7
- JCR IF
- JCR 2010 0.478
- ISSN
- 0374-4884
저자
- He, W제1저자부산대학교, KO
- 박세정부산대학교, KO
- Shin, Dong-Hyun부산대학교, BK Nano Fus Technol Div 21, KO
- 윤수종부산대학교, 나노과학기술대학, 나노메카트로닉스공학과, KO
- Wu, Yongqing부산대학교, Res Ctr Dielectr & Adv Matter Phys, KO
- Qiu, Jijun부산대학교, Res Ctr Dielectr & Adv Matter Phys, KO
- 황윤회교신저자부산대학교, 나노과학기술대학, 나노에너지공학과, KO
- 김형국교신저자부산대학교, 나노과학기술대학, 나노에너지공학과, KO
- Kim, Beomkeun인제대학교, Sch Mech & Automot Engn, KO
초록
Self-aligned highly ordered TiO2 nanotube arrays were fabricated by anodic oxidation of titanium foil. The effect of annealing Ti foils on the morphologies and the growth behaviors of TiO2 nanotube arrays was systematically investigated. We found that the thermal pre-treatment could eliminate the residual stress in the as-fabricated Ti foil and was, thus, beneficial in narrowing the diameter distribution and improving the alignment of TiO2 nanotube arrays. Besides, the growth rate of well-aligned TiO2 nanotube arrays with a honeycomb structure increased with increasing annealing temperature. The structural improvement of TiO2 nanotube arrays was a result of a homogeneous distribution of the electric field, resulting from the elimination the residual stress in as-fabricated Ti foil after annealing.
키워드
TiO2ElectrochemicalAnodic nanotubeAnnealingPHOTOCATALYTIC ACTIVITYTITANIUMFILMS