Effects of Weaving Laser on Weld Microstructure and Crack for Al 6k21-T4 Alloy

문서 유형
연구출판물 · 학술지 논문
등재
SCIEScopus
저널 순위
JCR Q2
저널
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY27(1) · pp.93 · 2011
피인용
Web of Science 20
JCR IF
JCR 2010 0.759
ISSN
1005-0302

저자

  1. Kim, B. H.제1저자부산대학교, 공과대학, 재료공학부, KO
  2. 강남현부산대학교, 공과대학, 재료공학부, KO
  3. Oh, W. T.동의대학교, Dept Mat & Components Engn, KO
  4. Kim, C. H.한국생산기술연구원, Adv Joining Technol Team, KO
  5. Kim, J. H.한국생산기술연구원, Adv Joining Technol Team, KO
  6. Kim, Y. S.한국생산기술연구원, Div Dongnam Area Technol Serv, KO
  7. 박용호부산대학교, 공과대학, 재료공학부, KO

초록

For Al 6k21-T4 overlap weld joint, the shear-tensile strength by using the weaving laser was improved as compared to the case of linear laser. For the specimen of low strength, the porosity was distributed continuously along the intersection between the plates and fusion line. However, for the optimized welding condition, large oval-shaped porosities were located only in the advancing track of the concave part. Therefore, the continuity of cracks and porosities played a key role to determine the strength. And, the weaving width was also the important parameter to control the strength. Furthermore, the concave part had more significant hot and cold cracking in the weld and heat-affected zone (HAZ), respectively, than the convex part.

키워드

Weaving laserWeld microstructureVoidAl alloyMAGNETIC ARC OSCILLATIONFRICTION STIR WELDSMG-SIMECHANICAL-PROPERTIESALUMINUM-ALLOYSPARAMETERSWELDMENTSTOUGHNESSBEHAVIOR