JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY11(1) · pp.463 · 2011
피인용
Web of Science 1
JCR IF
JCR 2010 1.352
ISSN
1533-4880

저자

  1. Qiu, Jijun제1저자RCDAMP, Pusan National University, South Korea
  2. Li, XiaominState Key Laboratory of High Performance Ceramics and Superfine Microstructures, Shanghai Institute of Ceramics, Chinese Academy of Sciences, China
  3. Wu, YongqingRCDAMP, Pusan National University, South Korea
  4. He, WeizhenDepartment of Nano Materials Engineering, BK 21 Nano Fusion Technology Division, Pusan National University, South Korea
  5. 박세정Department of Nano Materials Engineering, BK 21 Nano Fusion Technology Division, Pusan National University, South Korea
  6. 박충열Department of Nano Materials Engineering, BK 21 Nano Fusion Technology Division, Pusan National University, South Korea
  7. 김형국교신저자RCDAMP, Pusan National University, South Korea
  8. 황윤회RCDAMP, Pusan National University, South Korea
  9. Zhao, JunliangSchool of Electrical and Electronic Engineering, Nanyang Technological University, Singapore
  10. Wang, YeSchool of Electrical and Electronic Engineering, Nanyang Technological University, Singapore
  11. Sun, XiaoweiSchool of Electrical and Electronic Engineering, Nanyang Technological University, Singapore

초록

Ultralong ZnO nanorod arrays with a length of 10 mu m were synthesized using a preheated hydrothermal-solution precursor, and their optical and electrical properties were studied using photoluminescence (PL) spectra and field effect transistors (FETs). The PL spectra showed ultraviolet, orange, and red emissions and had different temperature dependences with increasing temperature. The high-resolution photoluminescence spectra showed that the ultraviolet (UV) emission had different origins within different temperature ranges. The parameters describing the temperature dependence of the peak position shift, intensity, and full width at half maximum were evaluated using different models. After the fabrication of individual nanorod FETs, the ultralong ZnO NRs showed a clear n-type gate modulation with a typical electron concentration of 10(17) cm(-3) and a typical electron mobility of 35.7 cm(2)/V . s.

키워드

ZnO NanorodHydrothermalPhotoluminescenceField Effect TransistorsFIELD-EFFECT TRANSISTORMOLECULAR-BEAM EPITAXYZINC-OXIDE NANOSTRUCTURESTEMPERATURE-DEPENDENCEOXYGEN-PLASMAPHOTOLUMINESCENCEDEPOSITIONSINGLESEMICONDUCTORSCONDUCTIVITY