Effect of TiO2 buffer layer thickness on properties of ITZO films deposited on flexible substrate

문서 유형
연구출판물 · 학술대회 발표논문
등재
SCIEScopus
저널 순위
JCR Q1
저널
SURFACE & COATINGS TECHNOLOGY205 · pp.S312 · 2010
피인용
Web of Science 15
JCR IF
JCR 2009 1.793
ISSN
0257-8972

저자

  1. 권세훈제1저자Department of Materials Science and Engineering, Pusan National University, South Korea
  2. Kang, Y. M.Department of Materials Science and Engineering, Pusan National University, South Korea
  3. 조영래Department of Materials Science and Engineering, Pusan National University, South Korea
  4. Kim, S. H.Department of Naval Architecture and Ocean Engineering, School of Mechanical Engineering, INHA University, South Korea
  5. 송풍근교신저자Department of Materials Science and Engineering, Pusan National University, South Korea

초록

In-Sn-Zn-O (ITZO) films and a TiO2 buffer layer were deposited on PET substrates at room temperature by magnetron co-sputtering using two cathodes (DC, RF) and RF reactive sputtering at an O-2 flow ratio of 2%, respectively. After applying a TiO2 buffer layer, the ITZO/TiO2 films showed an amorphous structure with a resistivity that decreased with increasing TiO2 buffer layer thickness. The mechanical properties were highest at a TiO2 thickness of 5 nm, which was confirmed by the bending test and optical microscopy images of the cracks. The resistivity and transmittance of the ITZO film with a 5 nm thick TiO2 buffer were 6.55 x 10(-4)Omega cm and >75% at 550 nm, respectively. (C) 2010 Elsevier B.V. All rights reserved.

키워드

In-Sn-Zn-OFlexible displayBuffer layerReactive sputteringINDIUM-TIN OXIDEMAGNETRON COSPUTTERING SYSTEMTHIN-FILMSROOM-TEMPERATUREGLASS

식별자

WoS UID
000286343200063